• [wzg:title/]
Hastelloy C 276 Electrode For Flowmeter
Hastelloy electrodes for magnetic flow meter. The electrodes widely used for electromagnetic flow meter producing, we can customized according your requirements. 316L electrode , Titanium electrode ,Tantalum electrode ,Hastelloy-C electrode.
Read More
Hastelloy C22 Pipe fittings
Hastelloy C 22 Pipe fittings ( Short Radius Elbows , Long Radius Elbows , Concentric Reducers , Eccentric Reducers , Stub Ends , End Caps , Equal Tees , Weldolets , Pipe Nipples .) ASME/ANSI B16.9, ASME B16.28, MSS-SP-43, MSS SP-79 , Type Seamless / Welded / Fabricated . Hastelloy C-22 / UNS N06022 / DIN W. Nr. 2.4602
Read More
Hastelloy C 276 Pipe fittings
Hastelloy C 276 Pipe fittings ( Short Radius Elbows , Long Radius Elbows , Concentric Reducers , Eccentric Reducers , Stub Ends , End Caps , Equal Tees , Weldolets , Pipe Nipples .) ASME/ANSI B16.9, ASME B16.28, MSS-SP-43, MSS SP-79 , Type Seamless / Welded / Fabricated Hastelloy C276 Pipe Fittings UNS (N10276), DIN (2.4819).
Read More
Inconel 625 Rod
Inconel Round Bar , ASTM B446 Inconel, 625 Bright Round Rod , Inconel 625 Hex Rods ,Inconel 625 flat bar with standard ASTM B446 / ASME SB446 and Nickel Alloy 625/ Inconel 625 (AMS 5666)
Read More
Inconel 601 Welding Wire
Inconel 601 Welding Wire - UNS N06601 - DIN W. Nr.2.4851 . ERNiCrFe-11 (Alloy 601) . ASME II, Part C, SFA-5.14, ERNiCrFe-11 (UNS N06601) , ASME IX, F-No.43 , BS290] NA 49 , DIN 1736 SG-NiCr23Al (2.4626) , (EN) ISO 18274 - SN16601 (NiCr23Fel5Al) , ASME III (NCA3800, NB2400), AMS and other specifications
Read More
Inconel 600 Welding Wire
Inconel 600 Wire ASTM B166 , Inconel 600 welding wire Alloy 600. UNS N06600 / W.Nr. 2.4816 .Nickel Alloy (AWS A5.11) ENiCrFe-3 Welding Electrode, Nickel Alloy ENiCrFe-3 Welding Electrode, ENiCrFe-3 inconel 600
Read More
Invar 32 Wire
Invar 32 Wire Super-Invar 32-5 rod UNS-K-93500, Consisting of 32% Nickel, 5% Cobalt, and the balance Iron, this alloy exhibits minimum thermal expansion (one half of Invar 36) at room temperature. It is often used in structural components, supports and substrates requiring precision measurements. ASTM F1684.
Read More
Invar 32 Sheet
Invar 32 Sheet, plate , Invar Alloy Foil , Super Invar 32-5 Alloy DESCRIPTION. A low expansion alloy consisting of 32% Nickel, 5% Cobalt, balance Iron. This alloy exhibits minimum thermal expansion (one half of Invar 36) Invar-36, Invar-42, Pernifer 36, Invar Steel, Super Invar 32-5, Carpenter 36, 4J32, 4J36
Read More
Invar 36 Plate
Alloy 36 Sheet (Invar) / K93603 / ASTM F1684 Widely known under several trades names such as Invar and Nilo 36**, this grade is a 36% nickel-iron alloy. AMS l-23011 CL7MIL l-23011 CL7UNS K93602/03 4J36 (China), Fe-Ni36 (France), 1.3912, Ni36 (Germany), X1NiCrMoCu, N 25-20-7 (UK) Invar 36, UNSK93600 thermostat alloy, UNSK93601 pressure vessel sheet (USA)
Read More
Alloy 46 Wire
Alloy 46 wire : Consisting of 46% nickel and iron balance, 46 Alloy is a controlled expansion alloy used mostly in electronic applications, especially for glass and ceramic seals. Alloy 46 is also known as Pernifer 462, NILO 464, and Glass-Seal 461 , ,Fe46Ni
Read More
Alloy 46 Sheet
Alloy 46: Consisting of 46% nickel and iron balance, 46 Alloy is a controlled expansion alloy used mostly in electronic applications, especially for glass and ceramic seals. Alloy 46 is also known as Pernifer 462, NILO 464, and Glass-Seal 461
Read More
MP35N Thread Bolt Fastener
MP35N Thread Rod , MP35N bolts , MP35N fasteners , UNS R30035 bolts , MP35N Thread Bar, MP35N Specifications: AMS 5844, AMS 5845, AMS7468, ASTM F562, NACE MR0175. MP35N alloys are used in fasteners, springs, non-magnetic assemblies and instrumentation components in medical, marine, oil and gas well, chemical and food processing environments.
Read More

Request a quote

Pure Molybdenum Heat Shield Polished Molybdneum Bars China

China % Pure HotRolled Polished Molybdenum Sheets/Plate

China % Pure Hot-Rolled Polished Molybdenum Sheets/Plate for Heat Shield with Factory Price, Find details about China Molybdenum Sheets, Heating Shield from % Pure Hot-Rolled Polished Molybdenum Sheets/Plate for Heat Shield with Factory Price - Luoyang Dingding Tungsten and Molybdenum Materials ,

China Vacuum Furnace Molybdenum Screen Heat Shield Radiation

Type: welding heat shield, riveting heat shield Heat shields panels and packs are manufactured for purpose of thermal insulation and reflection in a high temperature vacuum furnace. Depending on different furnace temperature, we can provide heat shields made of % pure molybdenum, MoLa and tungsten.

Molybdenum Heat Shield China Manufacturers Suppliers Factory

Our goal is 100% client gratification by our solution high-quality, rate and take pleasure in a great popularity among clients. With several factories, we will provide a wide assortment of Molybdenum Heat Shield, Molybdenum Heat Shield Parts, Molybdenum Heater, to forge a fantastic long term by our cooperation.

Molybdenum Heat Shield,Molybdenum Crucible,High Quality

Product categories of Molybdenum Products, we are specialized manufacturers from China, Molybdenum Heat Shield, Molybdenum Crucible suppliers/factory, wholesale high-quality products of Molybdenum Bar R D and manufacturing, we have the perfect after-sales service and technical support.

China Vacuum Furnace Molybdenum Heat Shield molybdenum

China Vacuum Furnace Molybdenum Heat Shield Molybdenum Disulfide Hot Sale % Molybdenum Price For Sheets/crucible , Find Complete Details about China Vacuum Furnace Molybdenum Heat Shield Molybdenum Disulfide Hot Sale % Molybdenum Price For Sheets/crucible,Molybdenum Disulfide,Polished Molybdenum Bar,Ferro Molybdenum from Molybdenum Supplier or Manufacturer-Luoyang Kekai Tungsten

Polished Pure Molybdenum Sheet Molybdenum Plate Buy Pure

Polished Pure Molybdenum Sheet Molybdenum Plate , Find Complete Details about Polished Pure Molybdenum Sheet Molybdenum Plate,Pure Molybdenum Sheet,Polished Molybdenum Plate,Molybdenum Sheet from Molybdenum Supplier or Manufacturer-Luoyang Sheng Ke Tungsten Molybdenum Technology ,

China Molybdenum Products Made by % Pure Molybdenum

Molybdenum, Pure Molybdenum, % Pure Molybdenum manufacturer / supplier in China, offering Molybdenum Products Made by % Pure Molybdenum, Chinese Tractor Spare Parts Steering Wheel Assembly, Chinese Tractor Spare Parts Orifice Cover and so on.

Pure Molybdenum Suppliers, all Quality Pure Molybdenum

Pure Molybdenum, Pure Molybdenum Suppliers Directory - Find variety Pure Molybdenum Suppliers, Manufacturers, Companies from around the World at guangming molybdenum wire ,molybdenum wire ,molybdenum bar, Molybdenum

molybdenum heat shields

offers 589 molybdenum heat shields products. such as free samples. There are 589 molybdenum heat shields suppliers, mainly located in Asia. The top supplying country or region is China, which supply 100% of molybdenum heat shields respectively.

China Molybdenum Shield, China Molybdenum Shield

China Molybdenum Shield, China Molybdenum Shield Suppliers and Manufacturers Directory - Source a Large Selection of Molybdenum Shield Products at sneaker shield ,captain america shield ,mica shield from China

China % Pure Polished Thickness Molybdenum

China % Pure Polished Thickness Molybdenum Sheets for Heat Shield, Find details about China Molybdenum Disk, Molybdenum Wafer from

Molybdenum Tungsten

9030 products % High Purity Various Dimensions Polishing Tungsten Tube/ Pipe Quality Polished % Tungsten Bars/Rods or Molybdenum Bars/Bars for Industry High Temperature % Molybdenum Heat Shield or Tungsten

China Hot Zone Manufacturer and Suppliers Hot Zone

Were a professional hot zone manufacturer and distributor in China. Molybdenum hot zone, Tungsten hot zone, Molybdenum heat shield, The main material for making a hot zone could be Molybdneum, Tungsten and their alloys. We can also manufacturing teat chamber made of Tantalum and Niobium bar/ sheet.

Tungsten bracket for sapphire growth furnaceChiantungsten

Molybdenum Heat Shield for Sapphire Growth Furnace The purity of tungsten bracket is over %, and its density is about /cm3, which Tungsten crucible cover and tungsten bracket can also be polished, which is showing the If there is any other question refer to tungsten and molybdenum for sapphire growth