• [wzg:title/]
Hastelloy C 276 Electrode For Flowmeter
Hastelloy electrodes for magnetic flow meter. The electrodes widely used for electromagnetic flow meter producing, we can customized according your requirements. 316L electrode , Titanium electrode ,Tantalum electrode ,Hastelloy-C electrode.
Read More
Hastelloy C22 Pipe fittings
Hastelloy C 22 Pipe fittings ( Short Radius Elbows , Long Radius Elbows , Concentric Reducers , Eccentric Reducers , Stub Ends , End Caps , Equal Tees , Weldolets , Pipe Nipples .) ASME/ANSI B16.9, ASME B16.28, MSS-SP-43, MSS SP-79 , Type Seamless / Welded / Fabricated . Hastelloy C-22 / UNS N06022 / DIN W. Nr. 2.4602
Read More
Hastelloy C 276 Pipe fittings
Hastelloy C 276 Pipe fittings ( Short Radius Elbows , Long Radius Elbows , Concentric Reducers , Eccentric Reducers , Stub Ends , End Caps , Equal Tees , Weldolets , Pipe Nipples .) ASME/ANSI B16.9, ASME B16.28, MSS-SP-43, MSS SP-79 , Type Seamless / Welded / Fabricated Hastelloy C276 Pipe Fittings UNS (N10276), DIN (2.4819).
Read More
Inconel 625 Rod
Inconel Round Bar , ASTM B446 Inconel, 625 Bright Round Rod , Inconel 625 Hex Rods ,Inconel 625 flat bar with standard ASTM B446 / ASME SB446 and Nickel Alloy 625/ Inconel 625 (AMS 5666)
Read More
Inconel 601 Welding Wire
Inconel 601 Welding Wire - UNS N06601 - DIN W. Nr.2.4851 . ERNiCrFe-11 (Alloy 601) . ASME II, Part C, SFA-5.14, ERNiCrFe-11 (UNS N06601) , ASME IX, F-No.43 , BS290] NA 49 , DIN 1736 SG-NiCr23Al (2.4626) , (EN) ISO 18274 - SN16601 (NiCr23Fel5Al) , ASME III (NCA3800, NB2400), AMS and other specifications
Read More
Inconel 600 Welding Wire
Inconel 600 Wire ASTM B166 , Inconel 600 welding wire Alloy 600. UNS N06600 / W.Nr. 2.4816 .Nickel Alloy (AWS A5.11) ENiCrFe-3 Welding Electrode, Nickel Alloy ENiCrFe-3 Welding Electrode, ENiCrFe-3 inconel 600
Read More
Invar 32 Wire
Invar 32 Wire Super-Invar 32-5 rod UNS-K-93500, Consisting of 32% Nickel, 5% Cobalt, and the balance Iron, this alloy exhibits minimum thermal expansion (one half of Invar 36) at room temperature. It is often used in structural components, supports and substrates requiring precision measurements. ASTM F1684.
Read More
Invar 32 Sheet
Invar 32 Sheet, plate , Invar Alloy Foil , Super Invar 32-5 Alloy DESCRIPTION. A low expansion alloy consisting of 32% Nickel, 5% Cobalt, balance Iron. This alloy exhibits minimum thermal expansion (one half of Invar 36) Invar-36, Invar-42, Pernifer 36, Invar Steel, Super Invar 32-5, Carpenter 36, 4J32, 4J36
Read More
Invar 36 Plate
Alloy 36 Sheet (Invar) / K93603 / ASTM F1684 Widely known under several trades names such as Invar and Nilo 36**, this grade is a 36% nickel-iron alloy. AMS l-23011 CL7MIL l-23011 CL7UNS K93602/03 4J36 (China), Fe-Ni36 (France), 1.3912, Ni36 (Germany), X1NiCrMoCu, N 25-20-7 (UK) Invar 36, UNSK93600 thermostat alloy, UNSK93601 pressure vessel sheet (USA)
Read More
Alloy 46 Wire
Alloy 46 wire : Consisting of 46% nickel and iron balance, 46 Alloy is a controlled expansion alloy used mostly in electronic applications, especially for glass and ceramic seals. Alloy 46 is also known as Pernifer 462, NILO 464, and Glass-Seal 461 , ,Fe46Ni
Read More
Alloy 46 Sheet
Alloy 46: Consisting of 46% nickel and iron balance, 46 Alloy is a controlled expansion alloy used mostly in electronic applications, especially for glass and ceramic seals. Alloy 46 is also known as Pernifer 462, NILO 464, and Glass-Seal 461
Read More
MP35N Thread Bolt Fastener
MP35N Thread Rod , MP35N bolts , MP35N fasteners , UNS R30035 bolts , MP35N Thread Bar, MP35N Specifications: AMS 5844, AMS 5845, AMS7468, ASTM F562, NACE MR0175. MP35N alloys are used in fasteners, springs, non-magnetic assemblies and instrumentation components in medical, marine, oil and gas well, chemical and food processing environments.
Read More

Request a quote

Molybdenum-Lanthanum Grind Support Rod

MolybdenumLanthanum Alloy Products SAM

We manufacture our molybdenum Lanthanum products according to your engineered drawing. Applications of Molybdenum Lanthanum . Molybdenum-lanthanum alloy is an ideal material for applications requiring dimensional stability and strength at temperatures above the capabilities of either pure Molybdenum or TZM alloy.

Molybdenum Lanthanum (MoLa) Alloy Bar / Rod ALB Materials Inc

Molybdenum Lanthanum (Mo-La) Alloy Bar / Rod Description: ALB Materials Inc is a global supplier of Molybdenum Lanthanum (Mo-La) Alloy Bar / Rod and we can provide customized molybdenum products.

Molybdenum Lanthanum (MoLa) Alloy Sheets ALB Materials Inc

ALB Materials Inc is a global supplier of Molybdenum Lanthanum (Mo-La) Alloy Bar / Rod and we can provide customized molybdenum products. Molybdenum Lanthanum alloy (Mo-La alloy) is an oxide dispersion strengthened alloy. Molybdenum Lanthanum (Mo-La) alloy is composed by adding lanthanum oxide in molybdenum.

Molybdenum Rods Bars Supplier Mosten Alloy ,

There are two types of molybdenum support rods: surface grinding and surface turning machining. We can manufacture molybdenum heating elements according to clients’ drawings. The purity of molybdenum support rods can reach 3N5, and density /cm 3.

Molybdenum Rods, Molybdenum Wires, Molybdenum Wire Rod

? Molybdenum Machined Rods Manufacturer ? Molybdenum Spraying Wire Suppliers ? Molybdenum Grind Rods Dealers ? Molybdenum Black Wires Stockyard ? Molybdenum lanthanum Rods Producer ? Molybdenum Precision Wire Exporter ? Moly Wire Rod Dealers Stockers ? Industrial Molybdenum wires Stockyards

Lanthanated Molybdenum Metal Elmet Technology

Lanthanated Molybdenum (Mo-La) In addition to pure and potassium doped (HCT) molybdenum, Elmet Technologies also produces lanthanated molybdenum products (Mo-La) such as rod, sheet, plate, and wire. Lanthanated molybdenum doped products have a higher recrystallization temperature than either pure molybdenum or HCT molybdenum, and they normally

Molybdenum Lanthanum

Molybdenum Lanthanum (Mo-La) is an alloy made by adding Lanthanum Oxide into molybdenum. Molybdenum Lanthanum has the properties of higher temperature of recrystallization, better ductility, and excellent wear-resistant. Molybdenum (Mo) is gray-metallic and has the third highest melting point of any element next to tungsten and tantalum.

High Temperature Moly Rod, Molybdenum Lanthanum Alloy Rod, Mo

High Temperature Moly Rod, Molybdenum Lanthanum Alloy Rod, Mo-La Bar High temperature molybdenum Rod containing La After add rare earth oxide containing La into molybdenum powder, re-crystallization temperature of products will raise notably, high temperature resistance performance and longer service life than pure molybdenum products.

. Starck Product Information Molybdendum Lanthanum (MoLa)

MOLYBDENUM LANTHANUM (Mo-La) Molybdenum Lanthanum is a molybdenum alloy containing Lanthanum Oxide. This oxide-dispersion strengthened molybdenum is a mixture of molybdenum with a very fine array/dispersion of lanthanum oxide particles.

ground molybdenum rods

offers 1,006 ground molybdenum rods products. About 66% of these are molybdenum, 1% are stainless steel bars, and 1% are other fiberglass products. A wide variety of ground molybdenum rods options are available to you, such as free samples.

Molybdenum Lanthanum (MoLa) Alloy Bar / Rod ALB

Molybdenum Lanthanum Alloy Bar / Rods, Mo-La Rods, MoLa Rods, Lanthanum Molybdenum Alloy, Mo-La Alloy Surface: Black, chemically cleaned, Grinding.

Molybdenum Sheet, Rod and Plate Electronic and Furnace

We can cut, slit, shear, or centerless grind Molybdenum to your exact tube grids and support structures that also require high temperature strength, low vapor

Molybdenum Rods Bars Supplier Mosten Alloy ,

There are two types of molybdenum support rods: surface grinding and surface rare earth lanthanum doped molybdenum and molybdenum rods are used.

Tungsten Plansee

WL-S is therefore the perfect material for support rods which have to maintain We dope tungsten with lanthanum oxide and zirconium oxide to obtain high creep .. Comminution, grinding, flotation and roasting processes can be employed to

Machining Guide to Molybdenum and Molybdenum Alloys

Molybdenum round bar sheet plate threaded rod Molybdenum (Mo), molybdenum lanthanum oxide (ML) and molybdenum Work should be firmly chucked; tools sharp and well supported; machines should be rigid, sufficiently powerful, and free from backlash. Wheel recommendations are indicated under grinding.

MolybdenumLanthanum Alloy Products SAM

MU0093 Mo-La Alloy (Molybdenum Lanthanum Alloy) Maximize. Inquiry - g/cc. Surface, Rolling surface, Chemical cleaned, Polished,Grinding

Molybdenum ThomasNet

Molybdenum, molybdenum-Tungsten alloy, tungsten in forms including rod, sheet, Capabilities include blanchard grinding up to 48-inches, surface grinding up to 96 distribution, inventory stocking, and other support services are provided. of Molybdenum, Molybdenum Lanthanum Oxide, TZM Molybdenum, Tungsten,

Applications of Molybdenum Metal and Its Alloys

provided strong support to organize reviewers and provide ore is processed in a series of grinding mill products like sheet, plate, foil, rod, “A Study of Welding Behavior for Molybdenum With and Without Lanthanum Oxide Additions, ”.

Molybdenum Machining Fabrication Elmet Technologies

Molybdenum Machining and Fabrication - With over 80 years of refractory metals stringent; machining and fabrication techniques must support demanding precision Tungsten Heavy Alloy Machining; Tantalum Alloy Machining; Lanthanum Alloy anodes and cathodes are machined from molybdenum and tungsten rod.

Molybdenum Lanthanum AlloyEdgetech Industries (A

Molybdenum Lanthanum alloy (Mo-La alloy) is one of the Moly-REO alloy Mo- La alloy sheet, plate, rod, bar and wire, machined parts for high temperature furnace are available. Surface, Black oxide, chemically cleaned, Grinding