• [wzg:title/]
Hastelloy C 276 Electrode For Flowmeter
Hastelloy electrodes for magnetic flow meter. The electrodes widely used for electromagnetic flow meter producing, we can customized according your requirements. 316L electrode , Titanium electrode ,Tantalum electrode ,Hastelloy-C electrode.
Read More
Hastelloy C22 Pipe fittings
Hastelloy C 22 Pipe fittings ( Short Radius Elbows , Long Radius Elbows , Concentric Reducers , Eccentric Reducers , Stub Ends , End Caps , Equal Tees , Weldolets , Pipe Nipples .) ASME/ANSI B16.9, ASME B16.28, MSS-SP-43, MSS SP-79 , Type Seamless / Welded / Fabricated . Hastelloy C-22 / UNS N06022 / DIN W. Nr. 2.4602
Read More
Hastelloy C 276 Pipe fittings
Hastelloy C 276 Pipe fittings ( Short Radius Elbows , Long Radius Elbows , Concentric Reducers , Eccentric Reducers , Stub Ends , End Caps , Equal Tees , Weldolets , Pipe Nipples .) ASME/ANSI B16.9, ASME B16.28, MSS-SP-43, MSS SP-79 , Type Seamless / Welded / Fabricated Hastelloy C276 Pipe Fittings UNS (N10276), DIN (2.4819).
Read More
Inconel 625 Rod
Inconel Round Bar , ASTM B446 Inconel, 625 Bright Round Rod , Inconel 625 Hex Rods ,Inconel 625 flat bar with standard ASTM B446 / ASME SB446 and Nickel Alloy 625/ Inconel 625 (AMS 5666)
Read More
Inconel 601 Welding Wire
Inconel 601 Welding Wire - UNS N06601 - DIN W. Nr.2.4851 . ERNiCrFe-11 (Alloy 601) . ASME II, Part C, SFA-5.14, ERNiCrFe-11 (UNS N06601) , ASME IX, F-No.43 , BS290] NA 49 , DIN 1736 SG-NiCr23Al (2.4626) , (EN) ISO 18274 - SN16601 (NiCr23Fel5Al) , ASME III (NCA3800, NB2400), AMS and other specifications
Read More
Inconel 600 Welding Wire
Inconel 600 Wire ASTM B166 , Inconel 600 welding wire Alloy 600. UNS N06600 / W.Nr. 2.4816 .Nickel Alloy (AWS A5.11) ENiCrFe-3 Welding Electrode, Nickel Alloy ENiCrFe-3 Welding Electrode, ENiCrFe-3 inconel 600
Read More
Invar 32 Wire
Invar 32 Wire Super-Invar 32-5 rod UNS-K-93500, Consisting of 32% Nickel, 5% Cobalt, and the balance Iron, this alloy exhibits minimum thermal expansion (one half of Invar 36) at room temperature. It is often used in structural components, supports and substrates requiring precision measurements. ASTM F1684.
Read More
Invar 32 Sheet
Invar 32 Sheet, plate , Invar Alloy Foil , Super Invar 32-5 Alloy DESCRIPTION. A low expansion alloy consisting of 32% Nickel, 5% Cobalt, balance Iron. This alloy exhibits minimum thermal expansion (one half of Invar 36) Invar-36, Invar-42, Pernifer 36, Invar Steel, Super Invar 32-5, Carpenter 36, 4J32, 4J36
Read More
Invar 36 Plate
Alloy 36 Sheet (Invar) / K93603 / ASTM F1684 Widely known under several trades names such as Invar and Nilo 36**, this grade is a 36% nickel-iron alloy. AMS l-23011 CL7MIL l-23011 CL7UNS K93602/03 4J36 (China), Fe-Ni36 (France), 1.3912, Ni36 (Germany), X1NiCrMoCu, N 25-20-7 (UK) Invar 36, UNSK93600 thermostat alloy, UNSK93601 pressure vessel sheet (USA)
Read More
Alloy 46 Wire
Alloy 46 wire : Consisting of 46% nickel and iron balance, 46 Alloy is a controlled expansion alloy used mostly in electronic applications, especially for glass and ceramic seals. Alloy 46 is also known as Pernifer 462, NILO 464, and Glass-Seal 461 , ,Fe46Ni
Read More
Alloy 46 Sheet
Alloy 46: Consisting of 46% nickel and iron balance, 46 Alloy is a controlled expansion alloy used mostly in electronic applications, especially for glass and ceramic seals. Alloy 46 is also known as Pernifer 462, NILO 464, and Glass-Seal 461
Read More
MP35N Thread Bolt Fastener
MP35N Thread Rod , MP35N bolts , MP35N fasteners , UNS R30035 bolts , MP35N Thread Bar, MP35N Specifications: AMS 5844, AMS 5845, AMS7468, ASTM F562, NACE MR0175. MP35N alloys are used in fasteners, springs, non-magnetic assemblies and instrumentation components in medical, marine, oil and gas well, chemical and food processing environments.
Read More

Request a quote

Molybdenum Disks/Molybdenum Squares

Molybdenum Disc,Molybdenum Square Supplier SAM

Description of Molybdenum Disc/Square Molybdenum is gray-metallic and has the third highest melting point of any element next to tungsten and tantalum. It is found in various oxidation states in minerals but does not occur naturally as a free metal.

. Starck Molybdenum Discs and Squares

Molybdenum Discs and Squares Molybdenum discs and squares are widely used as materials in silicon controlled rectifier diodes, transistors and thyristors. Molybdenum has similar coefficients of thermal expansion (CTE) to silicon combined with moderate thermal conductivity, and are therefore suitable for large area power devices where considerable heat is generated.

MU0082 Molybdenum Disc Molybdenum Square Refractory

Molybdenum Disc. 7 ~ 100mm Diameter. ~ Thickness. Molybdenum Square. 25 ~ 100mm Width/Length. ~ Thickness. Flatness Tolerance. 4um. Roughness. Ra

Molybdenum Disc Stanford Materials

Product name: Molybdenum Discs/Squares Standard: ASTM B386 Material: Mo % Density: ~ /cc Application: Molybdenum Discs/Squares has a similar low coefficient of thermal expansion to that of silicon, and better machining properties.

Molybdenum Disc AEMMETAL

Molybdenum Discs/Squares has a similar low coefficient of thermal expansion to that of silicon, and better machining properties.

Molybdenum Disc Edgetech Industries (Advanced Materials

The standard package for molybdenum disc, TZM alloy disc, Mo-La disc is wooden crate, so that goods can be protected during handling and transportation. Small discs and squares will be appropriated packing in carton.

Molybdenum Disc Square

Description: Molybdenum is gray-metallic and has the third highest melting point of any element next to tungsten and tantalum. It is found in various oxidation states in minerals but does not occur naturally as a free metal. Molybdenum allows readily form hard and stable carbides. For this reason, M

Molybdenum DiscMolybdenum Products Manufacturer and Supplier

Molybdenum Discs The molybdenum discs have similar thermal expansion to silicon. They are widely used as materials in silicon controlled rectifier diodes, transistors and thyristors, mounting material for power semiconductor devices and heat sink bases.

Molybdenum Discs or Molybdenum Disks for Semiconductor

Molybdenum Discs or Molybdenum Disks for Semiconductor KK-06 - KK Products Made In China, China Manufacturer. Description: Product name: Molybdenum Disks/Squares Standard: ASTM B386 Material: Mo % Density: ~/cc Application: Molybdenum Discs/Squares has a similar low coefficient of thermal expansion to that of silicon, and better machining properties.

KK Brand Molybdenum discs/Molybdenum square/Moly disk/Moly

SELL KK Brand Molybdenum discs/Molybdenum square/Moly disk/Moly square

Molybdenum Disc,Molybdenum Square Supplier SAM

Description of Molybdenum Disc/Square. Molybdenum is gray-metallic and has the third highest melting point of any element next to tungsten and tantalum. It is found in various oxidation states in minerals but does not occur naturally as a free metal. Molybdenum allows readily to form hard and stable carbides. For this reason, Molybdenum is

. Starck Molybdenum Discs and Squares

Molybdenum discs and squares are widely used as materials in silicon controlled rectifier diodes, transistors and thyristors. Molybdenum has similar coefficients of thermal expansion (CTE) to silicon combined with moderate thermal conductivity, and are therefore suitable for large area power devices where considerable heat is generated.

MU0082 Molybdenum Disc Molybdenum Square Refractory Metals and Alloys

Descriptions of Molybdenum Disc s requirements, as well as square and other fabricated parts. The polishing surface and lapping surface are both available.

Molybdenum Disc AEMMETAL

Application: Molybdenum Discs/Squares has a similar low coefficient of thermal expansion to that of silicon, and better machining properties. For that reason, it’s usually used for heat dissipation as electronic component of high power and high reliability semiconductor, materials in silicon controlled rectifiers diodes, transistors and thyristors (GTO’S), mounting material for power semiconductor£?heat sink bases in IC’S, LSI’S and hybrid circuits.

Molybdenum Disc Stanford Materials

Product name: Molybdenum Discs/Squares Standard: ASTM B386 Material: Mo % Density: ~ /cc Application: Molybdenum Discs/Squares has a similar low coefficient of thermal expansion to that of silicon, and better machining properties. For that reason, its usually used for heat dissipation as electronic component of high power and

Molybdenum Disc Edgetech Industries (Advanced Materials Supplier)

Molybdenum Disc Square has a similar low coefficient of thermal expansion to with silicon, but better machining properties. Based on this reason, it is usually used for heat dissipation as electronic component of high power and high reliability semiconductor, materials in silicon controlled rectifiers diodes, transistors and thyristors (GTO), mounting material for power semiconductor, heat sink bases in IC, LSI and hybrid circuits.

Molybdenum Disc Molybdenum Square (Mo Disc Mo Square)

Heeger Materials (HM) provides customized Molybdenum Disc Molybdenum Square rod with the shortest lead time and the best price.

Molybdenum Disc TRM Refractory Material Specialist

TRM Molybdenum Disc/Square, Surface Roughness Ra , Purity %, semiconductor devices materials. Get quote now! sales@

Tungsten Sheet Molybdenum Disc YHG Metalaluminumcopperbrass

Tungsten sheets and molybdenum round (or square) sheets (or moly wafers/ molybdenum discs/disks) have similar thermal expansion rate to silicon and excellent mechanical strength, so they are suitable for semiconductor components heat dissipating materials with high power and high-reliability requirements, and also used for various machining like stamping.

Molybdenum Products Molybdenum Round Bar Manufacturer from Mumbai

We Pearl Overseas have Molybdenum Round bar in % Purity, We also offer Molybdenum Round Bar with ASTM Molybdenum Round Bar B387 standard. Molybdenum round bar is made as arbitrary length pieces or slice to clients craved lengths in widths running from inches to inches.