• [wzg:title/]
Hastelloy C 276 Electrode For Flowmeter
Hastelloy electrodes for magnetic flow meter. The electrodes widely used for electromagnetic flow meter producing, we can customized according your requirements. 316L electrode , Titanium electrode ,Tantalum electrode ,Hastelloy-C electrode.
Read More
Hastelloy C22 Pipe fittings
Hastelloy C 22 Pipe fittings ( Short Radius Elbows , Long Radius Elbows , Concentric Reducers , Eccentric Reducers , Stub Ends , End Caps , Equal Tees , Weldolets , Pipe Nipples .) ASME/ANSI B16.9, ASME B16.28, MSS-SP-43, MSS SP-79 , Type Seamless / Welded / Fabricated . Hastelloy C-22 / UNS N06022 / DIN W. Nr. 2.4602
Read More
Hastelloy C 276 Pipe fittings
Hastelloy C 276 Pipe fittings ( Short Radius Elbows , Long Radius Elbows , Concentric Reducers , Eccentric Reducers , Stub Ends , End Caps , Equal Tees , Weldolets , Pipe Nipples .) ASME/ANSI B16.9, ASME B16.28, MSS-SP-43, MSS SP-79 , Type Seamless / Welded / Fabricated Hastelloy C276 Pipe Fittings UNS (N10276), DIN (2.4819).
Read More
Inconel 625 Rod
Inconel Round Bar , ASTM B446 Inconel, 625 Bright Round Rod , Inconel 625 Hex Rods ,Inconel 625 flat bar with standard ASTM B446 / ASME SB446 and Nickel Alloy 625/ Inconel 625 (AMS 5666)
Read More
Inconel 601 Welding Wire
Inconel 601 Welding Wire - UNS N06601 - DIN W. Nr.2.4851 . ERNiCrFe-11 (Alloy 601) . ASME II, Part C, SFA-5.14, ERNiCrFe-11 (UNS N06601) , ASME IX, F-No.43 , BS290] NA 49 , DIN 1736 SG-NiCr23Al (2.4626) , (EN) ISO 18274 - SN16601 (NiCr23Fel5Al) , ASME III (NCA3800, NB2400), AMS and other specifications
Read More
Inconel 600 Welding Wire
Inconel 600 Wire ASTM B166 , Inconel 600 welding wire Alloy 600. UNS N06600 / W.Nr. 2.4816 .Nickel Alloy (AWS A5.11) ENiCrFe-3 Welding Electrode, Nickel Alloy ENiCrFe-3 Welding Electrode, ENiCrFe-3 inconel 600
Read More
Invar 32 Wire
Invar 32 Wire Super-Invar 32-5 rod UNS-K-93500, Consisting of 32% Nickel, 5% Cobalt, and the balance Iron, this alloy exhibits minimum thermal expansion (one half of Invar 36) at room temperature. It is often used in structural components, supports and substrates requiring precision measurements. ASTM F1684.
Read More
Invar 32 Sheet
Invar 32 Sheet, plate , Invar Alloy Foil , Super Invar 32-5 Alloy DESCRIPTION. A low expansion alloy consisting of 32% Nickel, 5% Cobalt, balance Iron. This alloy exhibits minimum thermal expansion (one half of Invar 36) Invar-36, Invar-42, Pernifer 36, Invar Steel, Super Invar 32-5, Carpenter 36, 4J32, 4J36
Read More
Invar 36 Plate
Alloy 36 Sheet (Invar) / K93603 / ASTM F1684 Widely known under several trades names such as Invar and Nilo 36**, this grade is a 36% nickel-iron alloy. AMS l-23011 CL7MIL l-23011 CL7UNS K93602/03 4J36 (China), Fe-Ni36 (France), 1.3912, Ni36 (Germany), X1NiCrMoCu, N 25-20-7 (UK) Invar 36, UNSK93600 thermostat alloy, UNSK93601 pressure vessel sheet (USA)
Read More
Alloy 46 Wire
Alloy 46 wire : Consisting of 46% nickel and iron balance, 46 Alloy is a controlled expansion alloy used mostly in electronic applications, especially for glass and ceramic seals. Alloy 46 is also known as Pernifer 462, NILO 464, and Glass-Seal 461 , ,Fe46Ni
Read More
Alloy 46 Sheet
Alloy 46: Consisting of 46% nickel and iron balance, 46 Alloy is a controlled expansion alloy used mostly in electronic applications, especially for glass and ceramic seals. Alloy 46 is also known as Pernifer 462, NILO 464, and Glass-Seal 461
Read More
MP35N Thread Bolt Fastener
MP35N Thread Rod , MP35N bolts , MP35N fasteners , UNS R30035 bolts , MP35N Thread Bar, MP35N Specifications: AMS 5844, AMS 5845, AMS7468, ASTM F562, NACE MR0175. MP35N alloys are used in fasteners, springs, non-magnetic assemblies and instrumentation components in medical, marine, oil and gas well, chemical and food processing environments.
Read More

Request a quote

Molybdenum Alloy Tzm Jigs And Fixture For Heater

TZM Molybdenum Alloy Physical Chemical Properties

TZM is an acronym for titanium-zirconium-molybdenum and is typically manufactured by powder metallurgy or arc-casting is an alloy that has a higher recrystallization temperature, higher creep strength, and higher tensile strength than pure, unalloyed molybdenum.

Moly, MoLa, TZM, Tungsten Other Alloys CeraMaterials

Refer to alloys of Molybdenum such as Mola and TZM listed below. Our office stocks commonly requested Moly and TZM parts, but if you need an item not listed or a metric size please us directly for a custom quote. What is TZM? Titanium-Zirconium-Molybdenum alloy, also known as TZM, contains % Titanium, % Zirconium, and % Carbon.

Alloy Molybdenum Products Properties

Pure Alloy Molybdenum TZM Molybdenum is available in wire, bar, rod, sheet, vacuum furnace components, heat shields, crucibles and more!

TZM AllThread TZM Threaded Rods Ready to Ship

The alloy is stronger than pure molybdenum and possesses a higher recrystallization temperature and better creep resistance. Commonly used in applications involving demanding mechanical loads, the recommended temperature is between 700℃ 1400℃. TZM All-Thread is stocked in 1/4″-20 x 36″.

Molybdenum Alloy Supplier Sheet, Plate, Wire, Tubes, Rods

Molybdenum’s prime alloy is TZM. This alloy contains % min. to % max. of Mo, % Ti and % Zr with a trace of C for carbide formations. TZM offers twice the strength of pure moly at temperatures over 1300°C. The recrystallization temperature of TZM is approximately 250°C higher than moly and it offers better weldability.

Molybdenum Plansee

MHC is a particle-reinforced molybdenum-based alloy which contains both hafnium and carbon. Thanks to the uniformly distributed, extremely fine carbides, the material benefits from outstanding heat and creep resistance and, at 1,550 °C, the maximum recommended temperature of use is 150 °C higher than that of TZM.

Molybdenum – Zormetal

For Molybdenum alloys, Zormetal offers a wide range of molybdenum and molybdenum alloy products. Molybdenum product types include sheet, plate, rod, wire and pipe. For Molybdenum product dimensions, please visit our stock page. TZM Molybdenum (Titanium – zirconium – molybdenum) TZM is a known molybdenum alloy (% Ti, % Zr, the

Molybdenum Molybdenum Alloys from Elmet Technologies

Molybdenum properties are unique which makes it desirable for use in a number of manufacturing industries. For example, with its high melting point, 2620°C, molybdenum can work as a load bearing material in industrial furnaces at temperatures ranging 1600°C and up to 2000 °C for certain other applications.

HeatTreat Rack Material Selection Based on Thermal

Molybdenum alloy (aka “moly”) typically refers to the TZM alloy of molybdenum. TZM contains Ti, Zr and carbon that form fine precipitates and give it high-temperature strength and durability. Moly can also refer to the Mo-La alloys, which are strengthened by fine La 2 O 3 precipitates instead of carbide precipitates. Again, for the purposes

Molybdenum Molybdenum Alloy Properties Eagle Alloys

When threading the thread depth should not be more than 50 to 60 percent because molybdenum tends to chip, Molybdenum can be rolled treaded. The molybdenum material and the die should be heated to approximately 325 degrees F. Molybdenum can be heated to 325 degrees F in air without the danger of oxidation.

TZM Molybdenum Alloy Molybdenum Products Properties

TZM is an acronym for titanium-zirconium-molybdenum and is typically manufactured by powder metallurgy or arc-casting is an alloy that has a higher recrystallization temperature, higher creep strength, and higher tensile strength than pure, unalloyed molybdenum.

Moly, MoLa, TZM, Tungsten Other Alloys CeraMaterials

TZM is manufactured from molybdenum by using small quantities of tiny, extremely fine carbides through P/M or Arc Casting technology. This alloy is a great high strength solution for high temperature applications. The alloy is stronger than pure molybdenum and possesses a higher recrystallization temperature and better creep resistance. Commonly used in applications involving demanding mechanical loads, it’s recommended use temperature is between 700℃ 1400℃.

Lanthanated Molybdenum :: Alloy Blend Purchase Online

Lanthanated Molybdenum, often referred to as MoLa or ML, is an alloy comprised of molybdenum (Mo) and lanthanum trioxide (La2O3) and often used in vacuum furnaces or other high heat applications due to its stability and creep resistance at temperatures above 2730oF (1500oC).. After recrystallization occurs due to the high temperatures, the ductility actually improves on account of the changes to the molybdenum grain structure from the lanthanum trioxide dispersion.

TZM (Titanium Zirconium Moly) molybdenum alloy

TZM alloy (Titanium Zirconium Molybdenum) at high temperatures compared to pure molybdenum has a higher recrystallization temperature and high strength and hardness. It also has a sufficient extension. Because dispersed in the matrix of the composite molybdenum carbide circular arc, which has excellent mechanical properties.

China Molybdenum Alloy Sheet/Plate (MoLa/TZM Mo copper) for Heating

China Molybdenum Alloy Sheet/Plate (MoLa/TZM Mo copper) for Heating Shield, Find details about China % Molybdenum Sheet, Molybdenum Plate from Molybdenum Alloy Sheet/Plate (MoLa/TZM Mo copper) for Heating Shield - Luoyang Huapei Tungsten Molybdenum Material ,

Product Information Tungsten, Molybdenum, Tantalum for . Starck

The hot zones in sapphire growing furnaces use . Starck’s molybdenum and tungsten products for furnace components and fixtures. These high temperature materials are characterized by their high thermal and electrical conductivity, low coefficient of thermal expansion, and excellent strength and stability at temperatures above 2,000°C.

Molybdenum (Mo) Chemical Properties Molybdenum Products

Heat-Resistant Properties. Molybdenum is an important alloying agent which contributes to the hardenability and toughness of quenched and tempered steels. It also improves the strength of steel at high temperatures. It is used in certain heat-resistant and corrosion-resistant nickel-based alloys.

Joining of Refractory Metals and its Application

molybedenum and the alloy TZM, good weldability is given for Mo41Re. A welding procedure was established and used for the manufacturing of thin walled tubes. Rotary friction welding experiments were carried out on rod material of the Mo-alloys TZM and MHC. Suitable process parameter were determined and successfully transferred for the joining of tubular TZM parts. Keywords Refractory metals, molybdenum, joining, EB-welding, friction welding Introduction Refractory metals such as Mo and W are

Molybdenum Plansee

MHC is a particle-reinforced molybdenum-based alloy which contains both hafnium and carbon. Thanks to the uniformly distributed, extremely fine carbides, the material benefits from outstanding heat and creep resistance and, at 1,550 °C, the maximum recommended temperature of use is 150 °C higher than that of TZM.

Molybdenum Machining Information Services Molybdenum Products

Molybdenum can be rolled threaded, but this method is slow, and the preferred, faster methods consist of turning or chasing. Heat the moly and the die to 162°C for best results. Molybdenum can be heated to 162°C in air without the danger of oxidation, but the temperature should not exceed 260°C except in protective atmospheres. While slower