• [wzg:title/]
Hastelloy C 276 Electrode For Flowmeter
Hastelloy electrodes for magnetic flow meter. The electrodes widely used for electromagnetic flow meter producing, we can customized according your requirements. 316L electrode , Titanium electrode ,Tantalum electrode ,Hastelloy-C electrode.
Read More
Hastelloy C22 Pipe fittings
Hastelloy C 22 Pipe fittings ( Short Radius Elbows , Long Radius Elbows , Concentric Reducers , Eccentric Reducers , Stub Ends , End Caps , Equal Tees , Weldolets , Pipe Nipples .) ASME/ANSI B16.9, ASME B16.28, MSS-SP-43, MSS SP-79 , Type Seamless / Welded / Fabricated . Hastelloy C-22 / UNS N06022 / DIN W. Nr. 2.4602
Read More
Hastelloy C 276 Pipe fittings
Hastelloy C 276 Pipe fittings ( Short Radius Elbows , Long Radius Elbows , Concentric Reducers , Eccentric Reducers , Stub Ends , End Caps , Equal Tees , Weldolets , Pipe Nipples .) ASME/ANSI B16.9, ASME B16.28, MSS-SP-43, MSS SP-79 , Type Seamless / Welded / Fabricated Hastelloy C276 Pipe Fittings UNS (N10276), DIN (2.4819).
Read More
Inconel 625 Rod
Inconel Round Bar , ASTM B446 Inconel, 625 Bright Round Rod , Inconel 625 Hex Rods ,Inconel 625 flat bar with standard ASTM B446 / ASME SB446 and Nickel Alloy 625/ Inconel 625 (AMS 5666)
Read More
Inconel 601 Welding Wire
Inconel 601 Welding Wire - UNS N06601 - DIN W. Nr.2.4851 . ERNiCrFe-11 (Alloy 601) . ASME II, Part C, SFA-5.14, ERNiCrFe-11 (UNS N06601) , ASME IX, F-No.43 , BS290] NA 49 , DIN 1736 SG-NiCr23Al (2.4626) , (EN) ISO 18274 - SN16601 (NiCr23Fel5Al) , ASME III (NCA3800, NB2400), AMS and other specifications
Read More
Inconel 600 Welding Wire
Inconel 600 Wire ASTM B166 , Inconel 600 welding wire Alloy 600. UNS N06600 / W.Nr. 2.4816 .Nickel Alloy (AWS A5.11) ENiCrFe-3 Welding Electrode, Nickel Alloy ENiCrFe-3 Welding Electrode, ENiCrFe-3 inconel 600
Read More
Invar 32 Wire
Invar 32 Wire Super-Invar 32-5 rod UNS-K-93500, Consisting of 32% Nickel, 5% Cobalt, and the balance Iron, this alloy exhibits minimum thermal expansion (one half of Invar 36) at room temperature. It is often used in structural components, supports and substrates requiring precision measurements. ASTM F1684.
Read More
Invar 32 Sheet
Invar 32 Sheet, plate , Invar Alloy Foil , Super Invar 32-5 Alloy DESCRIPTION. A low expansion alloy consisting of 32% Nickel, 5% Cobalt, balance Iron. This alloy exhibits minimum thermal expansion (one half of Invar 36) Invar-36, Invar-42, Pernifer 36, Invar Steel, Super Invar 32-5, Carpenter 36, 4J32, 4J36
Read More
Invar 36 Plate
Alloy 36 Sheet (Invar) / K93603 / ASTM F1684 Widely known under several trades names such as Invar and Nilo 36**, this grade is a 36% nickel-iron alloy. AMS l-23011 CL7MIL l-23011 CL7UNS K93602/03 4J36 (China), Fe-Ni36 (France), 1.3912, Ni36 (Germany), X1NiCrMoCu, N 25-20-7 (UK) Invar 36, UNSK93600 thermostat alloy, UNSK93601 pressure vessel sheet (USA)
Read More
Alloy 46 Wire
Alloy 46 wire : Consisting of 46% nickel and iron balance, 46 Alloy is a controlled expansion alloy used mostly in electronic applications, especially for glass and ceramic seals. Alloy 46 is also known as Pernifer 462, NILO 464, and Glass-Seal 461 , ,Fe46Ni
Read More
Alloy 46 Sheet
Alloy 46: Consisting of 46% nickel and iron balance, 46 Alloy is a controlled expansion alloy used mostly in electronic applications, especially for glass and ceramic seals. Alloy 46 is also known as Pernifer 462, NILO 464, and Glass-Seal 461
Read More
MP35N Thread Bolt Fastener
MP35N Thread Rod , MP35N bolts , MP35N fasteners , UNS R30035 bolts , MP35N Thread Bar, MP35N Specifications: AMS 5844, AMS 5845, AMS7468, ASTM F562, NACE MR0175. MP35N alloys are used in fasteners, springs, non-magnetic assemblies and instrumentation components in medical, marine, oil and gas well, chemical and food processing environments.
Read More

Request a quote

Modern Antique Tzm Molybdenum Sheets

TZM Molybdenum Alloy (Sheet, Bar, Powder)

Molybdenums prime alloy is TZM. This alloy contains % min. to % max. of Mo, % Ti and % Zr with a trace of C for carbide formations. TZM offers twice the strength of pure moly at temperatures over 1300°C. The recrystallization temperature of TZM is approximately 250°C higher than moly and it offers better weldability.

TZM Molybdenum Alloy Physical Chemical Properties

TZM Molybdenum TZM is an acronym for titanium-zirconium-molybdenum ?and is typically manufactured by powder metallurgy or arc-casting processes. It is an alloy that has a higher recrystallization temperature, higher creep strength, and higher tensile strength than pure, unalloyed molybdenum.

Data Sheet Molybdenum (Mo, TZM, ML) WHS Sondermetalle

Titanium-Zirconium-Molybdenum (TZM) TZM is a micro-alloyed Molybdenum with Titanium-Zirconium-Carbides ( % Ti, % Zr, % C). By means of solid-solution and carbide-strengthening TZM features improved high temperature strength up to 1400 °C and a higher recrystallization temperature, compared to pure Molybdenum.

Molybdenum Sheet Products Elmet Technologies

Elmet is a leading global provider of high-quality molybdenum sheet products and the only US owned and operated producer. Elmet offers a wide range of cold rolled sheet product in varying thickness and length and per customer request.

TZM Molybdenum Alloy Sheet AMERICAN ELEMENTS

TZM Molybdenum Alloy Sheet Ti Zr Mo bulk research qty manufacturer. Properties, SDS, Applications, Price. Free samples program. Term contracts credit cards/PayPal accepted.

Molybdenum Plansee

TZM is stronger than pure molybdenum and possesses a higher recrystallization temperature and better creep resistance. TZM is used in high-temperature applications involving demanding mechanical loads, for example in forging tools or as rotating anodes in X-ray tubes. The recommended temperatures of use are between 700 and 1,400 °C.

Molybdenum Molybdenum Alloys from Elmet Technologies

Molybdenum properties are unique which makes it desirable for use in a number of manufacturing industries. For example, with its high melting point, 2620°C, molybdenum can work as a load bearing material in industrial furnaces at temperatures ranging 1600°C and up to 2000 °C for certain other applications.

Mosten Alloy ,

Mosten Alloy , Leading Supplier of Molybdenum and Tungsten High Quality Reasonable Price Best Service Applications: Semiconductor, Solar Energy,

Molybdenum Supplier Sheet, Plate, Wire, Tubes, Rods

Molybdenum has been used for many years in the lamp industry for mandrels and supports, usually in wire form. Today, several unique properties of molybdenum that satisfy more demanding industry requirements have increased the use of molybdenum as a material in applications requiring other mill forms.

Molybdenum Alloy Plates, Sheets Rods Supplier Eagle

Molybdenum Properties Molybdenum Stock List Request a quote Eagle Alloys Corporation can supply commercially pure Molybdenum, TZM, Molybdenum Copper Alloys, Copper Cladded Molybdenum, and Molybdenum Rhenium Alloys in foil, strip, sheet, plate, wire, rod, bar, tubing, as well as finished parts, custom sizes, and custom grades.

Molybdenum Supplier Sheet, Plate, Wire, Tubes, Rods

Rembar has molybdenum wires, sheets, rods, tubing, and plates in stock and ready to ship. Modern Applications of Molybdenum As electronics moved from the world of vacuum tubes to solid-state devices, new applications replaced the old. Only dies and other components made from molybdenum TZM ( %

Molybdenum Plansee

Plansee is an expert for the production of molybdenum products. Molybdenum- copper-composites for the advanced thermal management of modern electronics From powder to a .. Typical tensile strength for Mo and TZM sheet material in

Molybdenum Sheet Products All Sizes Moly Sheet Made

Elmet is a leading global provider of high-quality molybdenum sheet products and the only US owned and operated producer. Elmet offers a wide range of cold

TZM Sheet Products Moly TZM All Sheet Sizes TZM Made

Elmet is a leading global provider of high-quality TZM Alloy (Titanium, Zirconium, Molybdenum) sheet products and the only US owned and operated producer.

TZM Molybdenum Alloy (Sheet, Bar, Powder)

Molybdenum alloy TZM is an alloy of molybdenum, titanium, zirconium and carbon. It has a higher recrystallization temperature, higher creep strength and

Molybdenum High Temperature Alloy TZM Sheet online

General Description: Increased high temperature strength over pure Molybdenum although, like Molybdenum, it oxidises rapidly in oxidising atmospheres above