• [wzg:title/]
Hastelloy C 276 Electrode For Flowmeter
Hastelloy electrodes for magnetic flow meter. The electrodes widely used for electromagnetic flow meter producing, we can customized according your requirements. 316L electrode , Titanium electrode ,Tantalum electrode ,Hastelloy-C electrode.
Read More
Hastelloy C22 Pipe fittings
Hastelloy C 22 Pipe fittings ( Short Radius Elbows , Long Radius Elbows , Concentric Reducers , Eccentric Reducers , Stub Ends , End Caps , Equal Tees , Weldolets , Pipe Nipples .) ASME/ANSI B16.9, ASME B16.28, MSS-SP-43, MSS SP-79 , Type Seamless / Welded / Fabricated . Hastelloy C-22 / UNS N06022 / DIN W. Nr. 2.4602
Read More
Hastelloy C 276 Pipe fittings
Hastelloy C 276 Pipe fittings ( Short Radius Elbows , Long Radius Elbows , Concentric Reducers , Eccentric Reducers , Stub Ends , End Caps , Equal Tees , Weldolets , Pipe Nipples .) ASME/ANSI B16.9, ASME B16.28, MSS-SP-43, MSS SP-79 , Type Seamless / Welded / Fabricated Hastelloy C276 Pipe Fittings UNS (N10276), DIN (2.4819).
Read More
Inconel 625 Rod
Inconel Round Bar , ASTM B446 Inconel, 625 Bright Round Rod , Inconel 625 Hex Rods ,Inconel 625 flat bar with standard ASTM B446 / ASME SB446 and Nickel Alloy 625/ Inconel 625 (AMS 5666)
Read More
Inconel 601 Welding Wire
Inconel 601 Welding Wire - UNS N06601 - DIN W. Nr.2.4851 . ERNiCrFe-11 (Alloy 601) . ASME II, Part C, SFA-5.14, ERNiCrFe-11 (UNS N06601) , ASME IX, F-No.43 , BS290] NA 49 , DIN 1736 SG-NiCr23Al (2.4626) , (EN) ISO 18274 - SN16601 (NiCr23Fel5Al) , ASME III (NCA3800, NB2400), AMS and other specifications
Read More
Inconel 600 Welding Wire
Inconel 600 Wire ASTM B166 , Inconel 600 welding wire Alloy 600. UNS N06600 / W.Nr. 2.4816 .Nickel Alloy (AWS A5.11) ENiCrFe-3 Welding Electrode, Nickel Alloy ENiCrFe-3 Welding Electrode, ENiCrFe-3 inconel 600
Read More
Invar 32 Wire
Invar 32 Wire Super-Invar 32-5 rod UNS-K-93500, Consisting of 32% Nickel, 5% Cobalt, and the balance Iron, this alloy exhibits minimum thermal expansion (one half of Invar 36) at room temperature. It is often used in structural components, supports and substrates requiring precision measurements. ASTM F1684.
Read More
Invar 32 Sheet
Invar 32 Sheet, plate , Invar Alloy Foil , Super Invar 32-5 Alloy DESCRIPTION. A low expansion alloy consisting of 32% Nickel, 5% Cobalt, balance Iron. This alloy exhibits minimum thermal expansion (one half of Invar 36) Invar-36, Invar-42, Pernifer 36, Invar Steel, Super Invar 32-5, Carpenter 36, 4J32, 4J36
Read More
Invar 36 Plate
Alloy 36 Sheet (Invar) / K93603 / ASTM F1684 Widely known under several trades names such as Invar and Nilo 36**, this grade is a 36% nickel-iron alloy. AMS l-23011 CL7MIL l-23011 CL7UNS K93602/03 4J36 (China), Fe-Ni36 (France), 1.3912, Ni36 (Germany), X1NiCrMoCu, N 25-20-7 (UK) Invar 36, UNSK93600 thermostat alloy, UNSK93601 pressure vessel sheet (USA)
Read More
Alloy 46 Wire
Alloy 46 wire : Consisting of 46% nickel and iron balance, 46 Alloy is a controlled expansion alloy used mostly in electronic applications, especially for glass and ceramic seals. Alloy 46 is also known as Pernifer 462, NILO 464, and Glass-Seal 461 , ,Fe46Ni
Read More
Alloy 46 Sheet
Alloy 46: Consisting of 46% nickel and iron balance, 46 Alloy is a controlled expansion alloy used mostly in electronic applications, especially for glass and ceramic seals. Alloy 46 is also known as Pernifer 462, NILO 464, and Glass-Seal 461
Read More
MP35N Thread Bolt Fastener
MP35N Thread Rod , MP35N bolts , MP35N fasteners , UNS R30035 bolts , MP35N Thread Bar, MP35N Specifications: AMS 5844, AMS 5845, AMS7468, ASTM F562, NACE MR0175. MP35N alloys are used in fasteners, springs, non-magnetic assemblies and instrumentation components in medical, marine, oil and gas well, chemical and food processing environments.
Read More

Request a quote

Hot Selling Molybdenum Hanger Bolt Target For X-Ray Detectors

Molybdenum Plansee

Thanks to the special forming processes we use, Plansees molybdenum sputtering targets have a density of almost 100 %. You benefit from a faster process due to higher sputtering speeds. The denser the molybdenum target is, the better the conductivity of the created layer.

XRay Tube Mo (Molybdenum) Klinger Educational Products

Directly heated hot cathode tube with screw thread for heat sink and two-pin plug socket for cathode heating for X-ray apparatus (554 800 / 554 801). Technical Data ? Anode material: molybdenum ? Characteristic radiation: Kα = pm ( keV), Kβ = pm ( keV) ? Max. emission current: 1 mA ? Max. anode vo

Copper vs Molybdenum Rigaku

Since the introduction of CCD based area detectors for X-ray crystallography molybdenum has often been put forward as the best choice for a general purpose diffractometer system. The ever-growing popularity of dual source systems has enabled many chemical crystallographers to gain experience with copper as well as molybdenum sources.

Molybdenum Sputtering Target Stanford Materials

Molybdenum sputtering target is widely used in manufacturing LCD and touch screens (panels). It is also used for solar cells and solar water heating. We can provide pure molybdenum and molybdenum alloy targets with different shapes, including disc, planar, rotary as well as custom targets.

Screws, rivets and bolts Plansee

Screws, rivets and bolts. We can supply you with rivets, screws and nuts made of molybdenum, tungsten, tantalum and niobium as well as a wide range of alloys that perfectly meet the needs of your project.

Molybdenum Products Properties

Molybdenum Products. We carry molybdenum in wire, rod, sheet, and plate. We also sell molybdenum nuts, bolts, heat shields, and other hardware for vacuum furnace and high vacuum environments. TZM alloy rod and plate are also available. Learn More

Molybdenum Price Per Kg, Wholesale Suppliers

offers 1,231 molybdenum price per kg products. About 58% of these are molybdenum, 26% are other metals metal products. A wide variety of molybdenum price per kg options are available to you, such as free samples. There are 1,231 molybdenum price per kg suppliers, mainly located in Asia.

Why does xray diffraction target material vary with small

Why does x-ray diffraction target material vary with small molecules and large molecules such as protein? And what are the target materials?.

Choice of Xray Target

Choice of X-ray Target. The wavelength, λ, of the characteristic line giving rise to a particular transition is given by Moseleys Law: 1 / λ = c (Z - σ) 2 where c and σ are constants, and Z is the atomic number of the metal used for the anode.

what is an tungsten target? Yahoo Answers

Best Answer: Tungsten target implies an X-Ray tube where high energy electrons are directed in a vacuum to strike a tungsten the electrons strike the tungsten very short wavelength X-rays are generated and pass out through the vacuum tube for use in medical diagnosis and engineering radiography of welds and castings has a very high melting point but it is nevertheless

Collimators for Xray detectors Plansee

We machine refractory metals such as tungsten, molybdenum and the tungsten heavy alloy Densimet ? , to produce highprecision collimators for X-ray detectors.

XRay Detection Using Amorphous Silicon Technology

material. Here, the instabilities in reverse current d u h g X-ray detection is limited to less than %. Various experimental studies of noise characteristics in Mo/a- Si:H Schottky .. Schernatic of the measurement circuit (top) and its equivalent noise cir- X-ray spectrum at a distance of 39 cm for tungsten target generated by.

The xray sensitivity of amorphous selenium for mammography.

A study of the x-ray sensitivity of amorphous selenium (a-Se) for digital The deposition procedure was identical to that used for a-Se flat-panel detectors. A high voltage was applied to the top surface of the a-Se layer in order to establish with 27 kVp spectra generated from an x-ray tube with a molybdenum (Mo) target.

A comparison of xray spectra and outputs from molybdenum

A comparison of x-ray spectra and outputs from molybdenum and tungsten targets. The relative merits of tungsten and molybdenum targets for mammography have been measured with a Ge(Li) detector and ion chamber respectively.

How should an X ray tube and detector be setup?

I have an X ray tube and a detector, but I have no idea how to set them up. I have Ag and Au target which filters should I use? A prominent example is mammography radiation and filtering (Mo anode, Mo filtering creates . Best wishes,.