• [wzg:title/]
Hastelloy C 276 Electrode For Flowmeter
Hastelloy electrodes for magnetic flow meter. The electrodes widely used for electromagnetic flow meter producing, we can customized according your requirements. 316L electrode , Titanium electrode ,Tantalum electrode ,Hastelloy-C electrode.
Read More
Hastelloy C22 Pipe fittings
Hastelloy C 22 Pipe fittings ( Short Radius Elbows , Long Radius Elbows , Concentric Reducers , Eccentric Reducers , Stub Ends , End Caps , Equal Tees , Weldolets , Pipe Nipples .) ASME/ANSI B16.9, ASME B16.28, MSS-SP-43, MSS SP-79 , Type Seamless / Welded / Fabricated . Hastelloy C-22 / UNS N06022 / DIN W. Nr. 2.4602
Read More
Hastelloy C 276 Pipe fittings
Hastelloy C 276 Pipe fittings ( Short Radius Elbows , Long Radius Elbows , Concentric Reducers , Eccentric Reducers , Stub Ends , End Caps , Equal Tees , Weldolets , Pipe Nipples .) ASME/ANSI B16.9, ASME B16.28, MSS-SP-43, MSS SP-79 , Type Seamless / Welded / Fabricated Hastelloy C276 Pipe Fittings UNS (N10276), DIN (2.4819).
Read More
Inconel 625 Rod
Inconel Round Bar , ASTM B446 Inconel, 625 Bright Round Rod , Inconel 625 Hex Rods ,Inconel 625 flat bar with standard ASTM B446 / ASME SB446 and Nickel Alloy 625/ Inconel 625 (AMS 5666)
Read More
Inconel 601 Welding Wire
Inconel 601 Welding Wire - UNS N06601 - DIN W. Nr.2.4851 . ERNiCrFe-11 (Alloy 601) . ASME II, Part C, SFA-5.14, ERNiCrFe-11 (UNS N06601) , ASME IX, F-No.43 , BS290] NA 49 , DIN 1736 SG-NiCr23Al (2.4626) , (EN) ISO 18274 - SN16601 (NiCr23Fel5Al) , ASME III (NCA3800, NB2400), AMS and other specifications
Read More
Inconel 600 Welding Wire
Inconel 600 Wire ASTM B166 , Inconel 600 welding wire Alloy 600. UNS N06600 / W.Nr. 2.4816 .Nickel Alloy (AWS A5.11) ENiCrFe-3 Welding Electrode, Nickel Alloy ENiCrFe-3 Welding Electrode, ENiCrFe-3 inconel 600
Read More
Invar 32 Wire
Invar 32 Wire Super-Invar 32-5 rod UNS-K-93500, Consisting of 32% Nickel, 5% Cobalt, and the balance Iron, this alloy exhibits minimum thermal expansion (one half of Invar 36) at room temperature. It is often used in structural components, supports and substrates requiring precision measurements. ASTM F1684.
Read More
Invar 32 Sheet
Invar 32 Sheet, plate , Invar Alloy Foil , Super Invar 32-5 Alloy DESCRIPTION. A low expansion alloy consisting of 32% Nickel, 5% Cobalt, balance Iron. This alloy exhibits minimum thermal expansion (one half of Invar 36) Invar-36, Invar-42, Pernifer 36, Invar Steel, Super Invar 32-5, Carpenter 36, 4J32, 4J36
Read More
Invar 36 Plate
Alloy 36 Sheet (Invar) / K93603 / ASTM F1684 Widely known under several trades names such as Invar and Nilo 36**, this grade is a 36% nickel-iron alloy. AMS l-23011 CL7MIL l-23011 CL7UNS K93602/03 4J36 (China), Fe-Ni36 (France), 1.3912, Ni36 (Germany), X1NiCrMoCu, N 25-20-7 (UK) Invar 36, UNSK93600 thermostat alloy, UNSK93601 pressure vessel sheet (USA)
Read More
Alloy 46 Wire
Alloy 46 wire : Consisting of 46% nickel and iron balance, 46 Alloy is a controlled expansion alloy used mostly in electronic applications, especially for glass and ceramic seals. Alloy 46 is also known as Pernifer 462, NILO 464, and Glass-Seal 461 , ,Fe46Ni
Read More
Alloy 46 Sheet
Alloy 46: Consisting of 46% nickel and iron balance, 46 Alloy is a controlled expansion alloy used mostly in electronic applications, especially for glass and ceramic seals. Alloy 46 is also known as Pernifer 462, NILO 464, and Glass-Seal 461
Read More
MP35N Thread Bolt Fastener
MP35N Thread Rod , MP35N bolts , MP35N fasteners , UNS R30035 bolts , MP35N Thread Bar, MP35N Specifications: AMS 5844, AMS 5845, AMS7468, ASTM F562, NACE MR0175. MP35N alloys are used in fasteners, springs, non-magnetic assemblies and instrumentation components in medical, marine, oil and gas well, chemical and food processing environments.
Read More

Request a quote

Hot Roll Molybdenum Plate Blank

Hot Rolling and Cold Rolling of Molybdenum Plate CHEMETAL USA

During the rolling process, a hydrogen-filled furnace provides a purified environment for the process of annealing the large size molybdenum plate. A regular size of finished cold rolled plate is about ~ x 700~800 x 2000~3000 mm. Therefore, the hot rolled plate used to roll to cold rolled plate needs to be much bigger in width, height and

Alloy Steel Grade 5 Plates, ASTM A387 Gr 5 Sheets, Gr 5 Coils

Stockist and Supplier of Alloy Steel Grade 5 Sheets in Dubai, Check price of ASTM A387 Gr 5 Shim Sheet in UAE, Huge stock of Chrome Molybdenum Gr 5 Hot Rolled Cold Rolled Plate at best price in Oman

Hot Rolled Molybdenum Plate, Hot Rolled Molybdenum Plate

We are Manufacturer, Supplier 36″) and with increased thickness capabilities (up to 3″).

Molybdenum Plate Products Elmet Technologies

Molybdenum Plate Products. Elmet is a global leader and the only US owned and operated manufacturer of molybdenum plate. Elmet offers high quality % pure molybdenum plate in standard plate thicknesses and with over $30 Million in recent capital investments we now also provide extra wide plate (36″) and with increased thickness capabilities (up to 3″).

Molybdenum Plate Weison Advanced Materials Co

Molybdenum Plate Applications. Molybdenum plate is widely used in die construction and furnace construction for spare electrical and semi-conductor industry, and vacuum furnace or high temperature furnace, thermal insulation material industry. Plate Size

Molybdenum Sheet Weison Advanced Materials Co

Molybdenum sheet is widely used in reflection shield, cover plate applied in the sapphire growth furnace, reflection shield, heating tape, connecting pieces applied in vacuum furnace, sputtering target applied in plasma coating film, and high temperature resistance boat.

Molybdenum Plate Stanford Materials

Material from .090 inches to 3 inches in thickness is classified as molybdenum plate. It is widely used in the construction of furnace tooling and parts and as a feed stock for the fabrication of parts for the electronics and semiconductor industries. Specification: We produce high quality molybdenum plate as one of our hot product.

Molybdenum sheets Plansee

Thanks to our high capacities, we can manufacture even very large quantities of molybdenum sheets without difficulty. Thanks to our state-of-the-art equipment and many years of experience in the field of powder metallurgy, we can guarantee that you receive top quality - in every molybdenum sheet we supply.

Molybdenum Sheet Products All Sizes Moly Sheet Made in

Elmet is a leading global provider of high-quality molybdenum sheet products and the only US owned and operated producer. Elmet offers a wide range of cold rolled sheet product in varying thickness and length and per customer request.

Molybdenum sheet, plate and foil . Starck

MOLYBDENUM PLATE, SHEET AND FOIL Vacuum Arc-Cast Molybdenum Mill Products. The VAC method of consolidation is unique to . Starck. Materials made by this process is available exclusively from . Starck and yields a homogeneous product which is very low in residual elements, provides better strength at elevated temperatures and exhibits excellent workability, weld-ability and good machining

Hot Rolling and Cold Rolling of Molybdenum Plate CHEMETAL USA

During the rolling process, a hydrogen-filled furnace provides a purified environment for the process of annealing the large size molybdenum plate. A regular size of finished cold rolled plate is about ~ x 700~800 x 2000~3000 mm. Therefore, the hot rolled plate used to roll to cold rolled plate needs to be much bigger in width, height and

Hot Rolled Molybdenum Plate, Hot Rolled Molybdenum Plate, Sintered

Hot Rolled Molybdenum Plate, Hot Rolled Molybdenum Plate, Sintered Molybdenum Sheet, Molybdenum Plate Manufacturer, Suppliers in Mumbai, India, Russia, Poland. We are Manufacturer, Supplier 36″) and with increased thickness capabilities (up to 3″). We can cut, size, or roll the

Hot Rolled Pure Molybdenum Sheet Plate Price Per Kg For

Hot Rolled Pure Molybdenum Sheet Plate Price Per Kg For Vacuum Furnace , Find Complete Details about Hot Rolled Pure Molybdenum Sheet Plate Price Per Kg For Vacuum Furnace,Molybdenum Plate,Molybdenum Plate,Molybdenum Sheet Plate Price Per Kg from Molybdenum Supplier or Manufacturer-Baoji Tianbo Metal Materials ,

molybdenum plate sheet, molybdenum plate sheet Suppliers and

offers 2,881 molybdenum plate sheet products. About 3% of these are Steel Sheets. A wide variety of molybdenum plate sheet options are available to you, such as technique, standard, and surface treatment.

Hot Rolled Molybdenum Plate manufacturers suppliers

China Hot Rolled Molybdenum Plate manufacturers - Select 2019 high quality Hot Rolled Molybdenum Plate products in best price from certified Chinese Stainless Steel Plate manufacturers, China Tungsten suppliers, wholesalers and factory on

Molybdenum Plate Weison Advanced Materials Co

Molybdenum Plate. We offer pure molybdenum plate, molybdenum plate blank, white molybdenum plate, black molybdenum plate, anneal molybdenum plate , TZM molybdenum plate , high temperature molybdenum plate , lanthanum molybdenum plate. Physical Chemical Properties. Purity:Mo ≥%. Density: ≥/cm3. Flatness: ≤2%. Tensile strength: 610 Mpa. Elongation:≥10%. Temperature : 1800°C - 2200°C. Surface: Hot rolled. Condition:Vacuum annealed and unannealed. Adaptation

Alloy Steel EN24 Sheet Plate, AISI 4340 Chromium Molybdenum Steel

Chromium Molybdenum Alloy Steel 4340 Sheets, AS 36CrNiMo4 CR Sheets, EN24 Steel Plate, DIN Hot Rolled Plate Stockist, ASTM A829 Alloy Structural Steel Plates, SNCM439 Alloy Steel Sheet, AISI 4340 Sheet, Alloy Steel Sheet Plate, 4340 Alloy Steel Plate Manufacturers in India, 4340 Sheet, Alloy Steel EN24 Plate Supplier in Mumbai, India.

Molybdenum sheet, plate and foil . Starck

MOLYBDENUM PLATE, SHEET AND FOIL Vacuum Arc-Cast Molybdenum Mill Products. The VAC method of consolidation is unique to . Starck. Materials made by this process is available exclusively from . Starck and yields a homogeneous product which is very low in residual elements, provides better strength at elevated temperatures and exhibits excellent workability, weld-ability and good machining characteristics.

Alloy Steel EN19 Sheet Plate, AISI 4140 Chromium Molybdenum Steel

Leading manufacturer, suppliers of EN19 Alloy Steel Plate, Alloy Steel 4140 Sheet, DIN Sheet, EN19 Steel Plate, 42CrMo4 Steel Sheets, AISI 4140 Structural Steel Plates, Chromium Molybdenum Alloy Steel SCM440 Hot Rolled Steel Plate in india.

Molybdenum Plate and Sheet Tungsten Molybdenum Metals

Molybdenum plate and sheet and molybdenum reflection shield are packed in plywood case and sent by ocean or air. Zhuzhou Jiabang Refractory Metal , was founded in 2008, specializing molybdenum products, such as molybdenum plate (molybdenum sheet). With rich experience, our products are in superior quality, gaining widespread recognition