• [wzg:title/]
Hastelloy C 276 Electrode For Flowmeter
Hastelloy electrodes for magnetic flow meter. The electrodes widely used for electromagnetic flow meter producing, we can customized according your requirements. 316L electrode , Titanium electrode ,Tantalum electrode ,Hastelloy-C electrode.
Read More
Hastelloy C22 Pipe fittings
Hastelloy C 22 Pipe fittings ( Short Radius Elbows , Long Radius Elbows , Concentric Reducers , Eccentric Reducers , Stub Ends , End Caps , Equal Tees , Weldolets , Pipe Nipples .) ASME/ANSI B16.9, ASME B16.28, MSS-SP-43, MSS SP-79 , Type Seamless / Welded / Fabricated . Hastelloy C-22 / UNS N06022 / DIN W. Nr. 2.4602
Read More
Hastelloy C 276 Pipe fittings
Hastelloy C 276 Pipe fittings ( Short Radius Elbows , Long Radius Elbows , Concentric Reducers , Eccentric Reducers , Stub Ends , End Caps , Equal Tees , Weldolets , Pipe Nipples .) ASME/ANSI B16.9, ASME B16.28, MSS-SP-43, MSS SP-79 , Type Seamless / Welded / Fabricated Hastelloy C276 Pipe Fittings UNS (N10276), DIN (2.4819).
Read More
Inconel 625 Rod
Inconel Round Bar , ASTM B446 Inconel, 625 Bright Round Rod , Inconel 625 Hex Rods ,Inconel 625 flat bar with standard ASTM B446 / ASME SB446 and Nickel Alloy 625/ Inconel 625 (AMS 5666)
Read More
Inconel 601 Welding Wire
Inconel 601 Welding Wire - UNS N06601 - DIN W. Nr.2.4851 . ERNiCrFe-11 (Alloy 601) . ASME II, Part C, SFA-5.14, ERNiCrFe-11 (UNS N06601) , ASME IX, F-No.43 , BS290] NA 49 , DIN 1736 SG-NiCr23Al (2.4626) , (EN) ISO 18274 - SN16601 (NiCr23Fel5Al) , ASME III (NCA3800, NB2400), AMS and other specifications
Read More
Inconel 600 Welding Wire
Inconel 600 Wire ASTM B166 , Inconel 600 welding wire Alloy 600. UNS N06600 / W.Nr. 2.4816 .Nickel Alloy (AWS A5.11) ENiCrFe-3 Welding Electrode, Nickel Alloy ENiCrFe-3 Welding Electrode, ENiCrFe-3 inconel 600
Read More
Invar 32 Wire
Invar 32 Wire Super-Invar 32-5 rod UNS-K-93500, Consisting of 32% Nickel, 5% Cobalt, and the balance Iron, this alloy exhibits minimum thermal expansion (one half of Invar 36) at room temperature. It is often used in structural components, supports and substrates requiring precision measurements. ASTM F1684.
Read More
Invar 32 Sheet
Invar 32 Sheet, plate , Invar Alloy Foil , Super Invar 32-5 Alloy DESCRIPTION. A low expansion alloy consisting of 32% Nickel, 5% Cobalt, balance Iron. This alloy exhibits minimum thermal expansion (one half of Invar 36) Invar-36, Invar-42, Pernifer 36, Invar Steel, Super Invar 32-5, Carpenter 36, 4J32, 4J36
Read More
Invar 36 Plate
Alloy 36 Sheet (Invar) / K93603 / ASTM F1684 Widely known under several trades names such as Invar and Nilo 36**, this grade is a 36% nickel-iron alloy. AMS l-23011 CL7MIL l-23011 CL7UNS K93602/03 4J36 (China), Fe-Ni36 (France), 1.3912, Ni36 (Germany), X1NiCrMoCu, N 25-20-7 (UK) Invar 36, UNSK93600 thermostat alloy, UNSK93601 pressure vessel sheet (USA)
Read More
Alloy 46 Wire
Alloy 46 wire : Consisting of 46% nickel and iron balance, 46 Alloy is a controlled expansion alloy used mostly in electronic applications, especially for glass and ceramic seals. Alloy 46 is also known as Pernifer 462, NILO 464, and Glass-Seal 461 , ,Fe46Ni
Read More
Alloy 46 Sheet
Alloy 46: Consisting of 46% nickel and iron balance, 46 Alloy is a controlled expansion alloy used mostly in electronic applications, especially for glass and ceramic seals. Alloy 46 is also known as Pernifer 462, NILO 464, and Glass-Seal 461
Read More
MP35N Thread Bolt Fastener
MP35N Thread Rod , MP35N bolts , MP35N fasteners , UNS R30035 bolts , MP35N Thread Bar, MP35N Specifications: AMS 5844, AMS 5845, AMS7468, ASTM F562, NACE MR0175. MP35N alloys are used in fasteners, springs, non-magnetic assemblies and instrumentation components in medical, marine, oil and gas well, chemical and food processing environments.
Read More

Request a quote

High Quality Molybdenum Crucible

Molybdenum Crucible a trusted supplier TNTI

Our molybdenum crucible is characterized by reliable quality, strong anti-oxidation and anticorrosion, high temperature resistance, quick heat conduction, high efficiency. With a working temperature among 1100℃, it’s applied in sapphire crystal growth, quartz glass melting, vacuum coating, rare earth smelting and other industries.

Molybdenum Crucible Available Best Quality At Lowest Price

Molybdenum Crucible: Good thermal conductivity and even heating are important crucible properties in transferring the heat from the interior of the furnance through the crucible to the metal charge. Crucibles with high graphite content in the carbon binder offer high thermal conductivity for fast melting in glass-fired furnaces.

Molybdenum Crucible Supplier SAM

Applications of Molybdenum Crucible With a high corrosion resistance to most acids and many molten materials such as glass or metals, molybdenum crucibles are ideal for the metallurgy, mechanism, and rare earth smelting industries. They can withstand vacuum thermal evaporation, nuclear fuel sintering, and capacitor sintering.

Molybdenum Crucibles Supplier Mosten Alloy ,

Sintered Molybdenum Crucible The density of sintered molybdenum crucibles is between /cm 3 and /cm 3. The density of the forged products is /cc. The purity is greater than 3N and the diameter of the moly crucible goes beyond 300mm.

Molybdenum Crucibles Molybdenum and Tungsten Products

Spin-Formed Crucibles. Large molybdenum plate blanks are hot spun formed to the specified product geometry; Elmet has experience in a wide variety of molybdenum crucible sizes up to 20″ diameter; Milled Crucibles. Material blanks are machined to the final product geometries; INCREASING QUALITY, YIELD, AND THROUGHPUT

China High Quality Molybdenum Crucible China Tungten

1The overall density of sintered molybdenum crucible is fairy high between 96gcm3 to 100gcm3 2Its chemical purity of sintered molybdenum crucible can be above 9995 3The diameter of sintered molybdenum crucible can be above 200mm

Molybdenum crucible

Due to the melting point of molybdenum is as high as 2610℃, so the molybdenum crucible is widely used in sapphire crystal growth furnace, quartz glass melting furnace, rare earth smelting furnace etc core container of the industrial furnace, its working temperature environment generally above 2000℃.

Molybdenum Heat Shield,Molybdenum Crucible,High Quality

Product categories of Molybdenum Products, we are specialized manufacturers from China, Molybdenum Heat Shield, Molybdenum Crucible suppliers/factory, wholesale high-quality products of Molybdenum Bar R D and manufacturing, we have the perfect after-sales service and technical support.

Molybdenum Crucible on sales Quality Molybdenum Crucible

high temperature % purity molybdenum pot for sale Product Name high temperature % purity molybdenum pot for sale Brand HUAXING Origin Shaanxi,China Apearance Molybdenum crucible/pot Application High

High Quality 9995 Molybdenum crucible Price for rare earth

High Quality 9995 Molybdenum crucible Price for rare earth smelting, US $ 40 - 75 / Kilogram, Shanxi, China, Kedipu, from Baoji Kedipu New Material , on .

Molybdenum Crucibles Elmet Technologies

Advanced Tungsten and Molybdenum parts for crystal growth applications. our customers with innovative, high-quality molybdenum and tungsten products.

Molybdenum Straight Wall Crucibles Alfa Aesar

Molybdenum is a refractory metal recognized for its excellent strength at high temperatures, its high melting point of 2610 C (4370 F) and its high resistance to

Pressed crucibles Plansee

Our pressed-sintered crucibles made of tungsten have a surface roughness of less than μm. The cycles run smoothly and deliver high-quality ingots.

Molybdenum Crucible Supplier SAM

Stanford Advanced Materials (SAM) is a leading supplier of high-quality molybdenum crucibles. With our customization capabilities and competitive prices, we

Molybdenum Crucibles AMERICAN ELEMENTS ?

Molybdenum Crucibles Mo bulk research qty manufacturer. It has the third highest melting point of any element, exceeded only by tungsten and tantalum.

Molybdenum Crucible online catalogue source supplier of

Molybdenum ( Mo ) - Crucible - Material Information Molybdenum has a high melting point and applications for the pure metal take advantage of this;

Molybdenum Crucible Stanford Materials

Molybdenum crucible is mainly used in metallurgy industry and mechanism used in crystalloid materials, and other burgeoning high technology industry.

Molybdenum cruciblemolybdneum products for sapphire

For the property of high melting point of tungsten crucible and molybdenum and high quality of the crystal, which can be produced high quality LED material.

The Use of Molybdenum and Tungsten in Crucibles AZoM

9 Jan 2013 Tungsten molybdenum crucibles perform well in the Heat Exchanger Method When sapphire is easily extracted, better yield and improved quality of They are also resistant to corrosion and have a high material density.

Molybdenum sheets / plates|. Corp.

Easier to be processed than tungsten and being a high melting point metal, these TEM, High quality molybdenum material that has overcome the disadvantages of Vapor deposition boat, Electron tubes, Furnace parts, Crucible, Standar

  • share:

Request a quote