• [wzg:title/]
Hastelloy C 276 Electrode For Flowmeter
Hastelloy electrodes for magnetic flow meter. The electrodes widely used for electromagnetic flow meter producing, we can customized according your requirements. 316L electrode , Titanium electrode ,Tantalum electrode ,Hastelloy-C electrode.
Read More
Hastelloy C22 Pipe fittings
Hastelloy C 22 Pipe fittings ( Short Radius Elbows , Long Radius Elbows , Concentric Reducers , Eccentric Reducers , Stub Ends , End Caps , Equal Tees , Weldolets , Pipe Nipples .) ASME/ANSI B16.9, ASME B16.28, MSS-SP-43, MSS SP-79 , Type Seamless / Welded / Fabricated . Hastelloy C-22 / UNS N06022 / DIN W. Nr. 2.4602
Read More
Hastelloy C 276 Pipe fittings
Hastelloy C 276 Pipe fittings ( Short Radius Elbows , Long Radius Elbows , Concentric Reducers , Eccentric Reducers , Stub Ends , End Caps , Equal Tees , Weldolets , Pipe Nipples .) ASME/ANSI B16.9, ASME B16.28, MSS-SP-43, MSS SP-79 , Type Seamless / Welded / Fabricated Hastelloy C276 Pipe Fittings UNS (N10276), DIN (2.4819).
Read More
Inconel 625 Rod
Inconel Round Bar , ASTM B446 Inconel, 625 Bright Round Rod , Inconel 625 Hex Rods ,Inconel 625 flat bar with standard ASTM B446 / ASME SB446 and Nickel Alloy 625/ Inconel 625 (AMS 5666)
Read More
Inconel 601 Welding Wire
Inconel 601 Welding Wire - UNS N06601 - DIN W. Nr.2.4851 . ERNiCrFe-11 (Alloy 601) . ASME II, Part C, SFA-5.14, ERNiCrFe-11 (UNS N06601) , ASME IX, F-No.43 , BS290] NA 49 , DIN 1736 SG-NiCr23Al (2.4626) , (EN) ISO 18274 - SN16601 (NiCr23Fel5Al) , ASME III (NCA3800, NB2400), AMS and other specifications
Read More
Inconel 600 Welding Wire
Inconel 600 Wire ASTM B166 , Inconel 600 welding wire Alloy 600. UNS N06600 / W.Nr. 2.4816 .Nickel Alloy (AWS A5.11) ENiCrFe-3 Welding Electrode, Nickel Alloy ENiCrFe-3 Welding Electrode, ENiCrFe-3 inconel 600
Read More
Invar 32 Wire
Invar 32 Wire Super-Invar 32-5 rod UNS-K-93500, Consisting of 32% Nickel, 5% Cobalt, and the balance Iron, this alloy exhibits minimum thermal expansion (one half of Invar 36) at room temperature. It is often used in structural components, supports and substrates requiring precision measurements. ASTM F1684.
Read More
Invar 32 Sheet
Invar 32 Sheet, plate , Invar Alloy Foil , Super Invar 32-5 Alloy DESCRIPTION. A low expansion alloy consisting of 32% Nickel, 5% Cobalt, balance Iron. This alloy exhibits minimum thermal expansion (one half of Invar 36) Invar-36, Invar-42, Pernifer 36, Invar Steel, Super Invar 32-5, Carpenter 36, 4J32, 4J36
Read More
Invar 36 Plate
Alloy 36 Sheet (Invar) / K93603 / ASTM F1684 Widely known under several trades names such as Invar and Nilo 36**, this grade is a 36% nickel-iron alloy. AMS l-23011 CL7MIL l-23011 CL7UNS K93602/03 4J36 (China), Fe-Ni36 (France), 1.3912, Ni36 (Germany), X1NiCrMoCu, N 25-20-7 (UK) Invar 36, UNSK93600 thermostat alloy, UNSK93601 pressure vessel sheet (USA)
Read More
Alloy 46 Wire
Alloy 46 wire : Consisting of 46% nickel and iron balance, 46 Alloy is a controlled expansion alloy used mostly in electronic applications, especially for glass and ceramic seals. Alloy 46 is also known as Pernifer 462, NILO 464, and Glass-Seal 461 , ,Fe46Ni
Read More
Alloy 46 Sheet
Alloy 46: Consisting of 46% nickel and iron balance, 46 Alloy is a controlled expansion alloy used mostly in electronic applications, especially for glass and ceramic seals. Alloy 46 is also known as Pernifer 462, NILO 464, and Glass-Seal 461
Read More
MP35N Thread Bolt Fastener
MP35N Thread Rod , MP35N bolts , MP35N fasteners , UNS R30035 bolts , MP35N Thread Bar, MP35N Specifications: AMS 5844, AMS 5845, AMS7468, ASTM F562, NACE MR0175. MP35N alloys are used in fasteners, springs, non-magnetic assemblies and instrumentation components in medical, marine, oil and gas well, chemical and food processing environments.
Read More

Request a quote

High Performance Molybdenum Crucible

HighPerformance Crucibles Sumitomo Electric USA

High-Performance Crucibles High-performance crucibles are the product of development in the pursuit of increased size and product life. In particular, molybdenum crucibles have been well-received as long-life crucibles due to such features as high density and uniform micro-structure. These are widely used for growing single-crystal sapphire.

Molybdenum Crucible Supplier SAM

Stanford Advanced Materials (SAM) is a leading supplier of high-quality molybdenum crucibles. With our customization capabilities and competitive prices, we are the first choice for many customers. Related products: Molybdenum Boat , Molybdenum Heating Elements , Molybdenum Electrode

Molybdenum Crucibles Molybdenum and Tungsten Products

Spin-Formed Crucibles. Large molybdenum plate blanks are hot spun formed to the specified product geometry; Elmet has experience in a wide variety of molybdenum crucible sizes up to 20″ diameter; Milled Crucibles. Material blanks are machined to the final product geometries; INCREASING QUALITY, YIELD, AND THROUGHPUT

. Starck Product Information Molybdenum Crucibles

MOLYBDENUM CRUCIBLES FOR SAPPHIRE CRYSTAL GROWTH (LED) IN HIGH TEMPERATURE FURNACES. The hot zones in sapphire growing furnaces use . Starck’s molybdenum and tungsten products for furnace components and fixtures. These high temperature materials are characterized by their high thermal and electrical conductivity, low coefficient of thermal expansion, and excellent strength and stability at temperatures above 2,000°C.

Molybdenum Spun Crucibles for LED Sapphire Crystal Growing

The high melting temperature and creep resistance of molybdenum are required to survive the harsh environment found in sapphire crystal growing. Molybdenum has a low thermal expansion coefficient (CTE), which is excellent for the design of the components in the sapphire growing furnace.

Molybdenum Crucible, Molybdenum Crucible Price AEMMETAL

Corrosion resistance, creep resistance, and high temperature performance make molybdenum and tungsten crucibles ideal for use in high temperature crystal growth processes. Crystal growth is at the foundation for many cutting edge technologies such as Sapphire touch screens, LED lighting parts, solar cells and high power lasers.

Molybdenum crucible

Due to the melting point of molybdenum is as high as 2610℃, so the molybdenum crucible is widely used in sapphire crystal growth furnace, quartz glass melting furnace, rare earth smelting furnace etc core container of the industrial furnace, its working temperature environment generally above 2000℃.

Crucible Liner, Molybdenum, 7cc, Temescal Telemark Style

Crucible Liner, Molybdenum, 7cc, Temescal s EC0007-3 are high purification molybdenum liners made to fit the standard Temescal and Telemark hearth. Our EC0007-3 moly liners have a Top ID of , a height of , a wall thickness of , and a 15 degree angle. Order from stock with savings.

Molybdenum Crucible Stanford Materials

Molybdenum crucible is mainly used in metallurgy industry and mechanism process industry, and it s a kind of indispensability material in rare earth smelting industry. Molybdenum crucibles are more frequently used in crystalloid materials, and other burgeoning high technology industry.

Crucible Tool Steel and Specialty Alloy General Information

For instance, M4 high speed steel’s chemical content is nearly identical to M2 high speed steel, except M4 contains 4% vanadium instead of 2%. Despite the high levels of molybdenum and tungsten carbides (about 6% tungsten, 5% molybdenum) in each grade, the small difference in vanadium content gives M4 nearly twice the wear life of M2 in many environments.

HighPerformance Crucibles Sumitomo Electric USA

High-performance crucibles are the product of development in the pursuit of increased size and product life. In particular, molybdenum crucibles have been

Molybdenum Straight Wall Crucibles Alfa Aesar

Molybdenum is a refractory metal recognized for its excellent strength at high temperatures, its high melting point of 2610 C (4370 F) and its high resistance to

Molybdenum Crucibles Elmet Technologies

Corrosion resistance, creep resistance, and high-temperature performance make molybdenum and tungsten crucibles ideal for use in high-temperature crystal

. Starck Product Information Molybdenum Crucibles

Molybdenum and Tungsten Crucibles – Powder Metallurgy. Pure Molybdenum ( % High Performance Solutions for the LED industry. Download PDF. cn.

Formed crucibles Plansee

Formed crucibles made of molybdenum and tungsten are the perfect vessels for melting and solidifying the Formed crucibles for the sapphire production.

Pressed crucibles Plansee

During sapphire production, the compound that is to become the future single crystal is melted in molybdenum and tungsten crucibles. It is in the in the field of powder metallurgy, we produce crucibles of a particularly high density and purity.

Molybdenum Crucibles AMERICAN ELEMENTS ?

American Elements specializes in supplying Molybdenum Crucibles Crucible Packaging, Lab Quantity with a variety of dimensions including round, in numerous

Molybdenum Lab Crucibles MTI Albany

Molybdenum Lab Crucibles. Superior strength at high temperatures. With a melting poing of 2610oC, molybdenum crucibles can be used for performing high

The Use of Molybdenum and Tungsten in Crucibles AZoM

9 Jan 2013 Tungsten molybdenum crucibles perform well in the Heat Exchanger source for high performance components made of refractory metals.

Molybdenum Crucible Supplier SAM

Stanford Advanced Materials (SAM) is a leading supplier of high-quality molybdenum crucibles. With our customization capabilities and competitive prices, we