• [wzg:title/]
Hastelloy C 276 Electrode For Flowmeter
Hastelloy electrodes for magnetic flow meter. The electrodes widely used for electromagnetic flow meter producing, we can customized according your requirements. 316L electrode , Titanium electrode ,Tantalum electrode ,Hastelloy-C electrode.
Read More
Hastelloy C22 Pipe fittings
Hastelloy C 22 Pipe fittings ( Short Radius Elbows , Long Radius Elbows , Concentric Reducers , Eccentric Reducers , Stub Ends , End Caps , Equal Tees , Weldolets , Pipe Nipples .) ASME/ANSI B16.9, ASME B16.28, MSS-SP-43, MSS SP-79 , Type Seamless / Welded / Fabricated . Hastelloy C-22 / UNS N06022 / DIN W. Nr. 2.4602
Read More
Hastelloy C 276 Pipe fittings
Hastelloy C 276 Pipe fittings ( Short Radius Elbows , Long Radius Elbows , Concentric Reducers , Eccentric Reducers , Stub Ends , End Caps , Equal Tees , Weldolets , Pipe Nipples .) ASME/ANSI B16.9, ASME B16.28, MSS-SP-43, MSS SP-79 , Type Seamless / Welded / Fabricated Hastelloy C276 Pipe Fittings UNS (N10276), DIN (2.4819).
Read More
Inconel 625 Rod
Inconel Round Bar , ASTM B446 Inconel, 625 Bright Round Rod , Inconel 625 Hex Rods ,Inconel 625 flat bar with standard ASTM B446 / ASME SB446 and Nickel Alloy 625/ Inconel 625 (AMS 5666)
Read More
Inconel 601 Welding Wire
Inconel 601 Welding Wire - UNS N06601 - DIN W. Nr.2.4851 . ERNiCrFe-11 (Alloy 601) . ASME II, Part C, SFA-5.14, ERNiCrFe-11 (UNS N06601) , ASME IX, F-No.43 , BS290] NA 49 , DIN 1736 SG-NiCr23Al (2.4626) , (EN) ISO 18274 - SN16601 (NiCr23Fel5Al) , ASME III (NCA3800, NB2400), AMS and other specifications
Read More
Inconel 600 Welding Wire
Inconel 600 Wire ASTM B166 , Inconel 600 welding wire Alloy 600. UNS N06600 / W.Nr. 2.4816 .Nickel Alloy (AWS A5.11) ENiCrFe-3 Welding Electrode, Nickel Alloy ENiCrFe-3 Welding Electrode, ENiCrFe-3 inconel 600
Read More
Invar 32 Wire
Invar 32 Wire Super-Invar 32-5 rod UNS-K-93500, Consisting of 32% Nickel, 5% Cobalt, and the balance Iron, this alloy exhibits minimum thermal expansion (one half of Invar 36) at room temperature. It is often used in structural components, supports and substrates requiring precision measurements. ASTM F1684.
Read More
Invar 32 Sheet
Invar 32 Sheet, plate , Invar Alloy Foil , Super Invar 32-5 Alloy DESCRIPTION. A low expansion alloy consisting of 32% Nickel, 5% Cobalt, balance Iron. This alloy exhibits minimum thermal expansion (one half of Invar 36) Invar-36, Invar-42, Pernifer 36, Invar Steel, Super Invar 32-5, Carpenter 36, 4J32, 4J36
Read More
Invar 36 Plate
Alloy 36 Sheet (Invar) / K93603 / ASTM F1684 Widely known under several trades names such as Invar and Nilo 36**, this grade is a 36% nickel-iron alloy. AMS l-23011 CL7MIL l-23011 CL7UNS K93602/03 4J36 (China), Fe-Ni36 (France), 1.3912, Ni36 (Germany), X1NiCrMoCu, N 25-20-7 (UK) Invar 36, UNSK93600 thermostat alloy, UNSK93601 pressure vessel sheet (USA)
Read More
Alloy 46 Wire
Alloy 46 wire : Consisting of 46% nickel and iron balance, 46 Alloy is a controlled expansion alloy used mostly in electronic applications, especially for glass and ceramic seals. Alloy 46 is also known as Pernifer 462, NILO 464, and Glass-Seal 461 , ,Fe46Ni
Read More
Alloy 46 Sheet
Alloy 46: Consisting of 46% nickel and iron balance, 46 Alloy is a controlled expansion alloy used mostly in electronic applications, especially for glass and ceramic seals. Alloy 46 is also known as Pernifer 462, NILO 464, and Glass-Seal 461
Read More
MP35N Thread Bolt Fastener
MP35N Thread Rod , MP35N bolts , MP35N fasteners , UNS R30035 bolts , MP35N Thread Bar, MP35N Specifications: AMS 5844, AMS 5845, AMS7468, ASTM F562, NACE MR0175. MP35N alloys are used in fasteners, springs, non-magnetic assemblies and instrumentation components in medical, marine, oil and gas well, chemical and food processing environments.
Read More

Request a quote

High Melting Point Molybdenum Plate For Sale

Molybdenum Alloy Plates, Sheets Rods Supplier Eagle

Molybdenum is a refractory metal that is commonly used as high temperature, corrosion resistant metal that can withstand high stress, high temperature ranges without greatly softening or expanding. Molybdenum has a melting point of 2,623 °C. Molybdenum is used for its extremely high melting point and relative flexibility.

Molybdenum Plate Products Elmet Technologies

Molybdenum Plate Products. Elmet is a global leader and the only US owned and operated manufacturer of molybdenum plate. Elmet offers high quality % pure molybdenum plate in standard plate thicknesses and with over $30 Million in recent capital investments we now also provide extra wide plate (36″) and with increased thickness capabilities (up to 3″).

Molybdenum Supplier Sheet, Plate, Wire, Tubes, Rods

Molybdenum is number 42 on the periodic table. With a melting point of 2610°C, molybdenum has a density of gm/cc. It has many properties that make it an excellent candidate for fabricated parts that must be made of a refractory metal. Molybdenum has been used for many years in the lamp industry for mandrels and supports, usually in wire

Molybdenum Plate AMERICAN ELEMENTS

Molybdenum is the 54th most abundant element in the earths crust. It has the third highest melting point of any element, exceeded only by tungsten and tantalum. Molybdenum does not occur naturally as a free metal, it is found in various oxidation states in minerals.

Cold Rolling Molybdenum Plate For High

Cold Rolling Molybdenum Plate For High Temperature Vacuum Furnace , Find Complete Details about Cold Rolling Molybdenum Plate For High Temperature Vacuum Furnace,Molybdenum Plate,Cold Rolling Molybdenum Plate,Molybdenum Plate For High Temperature Vacuum Furnace from Molybdenum Supplier or Manufacturer-Shaanxi Getwick Nonferrous Metals ,

Molybdenum Plansee

Molybdenum is a genuine all-rounder. We use this material, for example, to produce ribbons and wires for the lighting industry, semiconductor base plates for power electronics, glass melting electrodes, hot zones for high-temperature furnaces and sputtering targets for coating solar cells and flat screens.

High purity % Molybdenum plate Moly sputter target

High Purity % Molybdenum Plate Moly Sputter Target , Find Complete Details about High Purity % Molybdenum Plate Moly Sputter Target,Molybdenum Plate,Sputter Target,Ferro Molybdenum from Other Metals Metal Products Supplier or Manufacturer-Dengfeng Jinyu Thermoelectric Material ,

Buy Molybdenum Online

Molybdenum is an extremely hard metal, making it a useful alloying agent in the manufacture of high strength steels. It is one of the refractory metals which have very high melting points. This particularly increases the strength of these steels at high temperatures. Molybdenum is lustrous and silver, with many physical similarities to tungsten.

High Temperature Mo La Molybdenum Foils For Sale Buy

High Temperature Mo La Molybdenum Foils For Sale , Find Complete Details about High Temperature Mo La Molybdenum Foils For Sale,Molybdenum Foil,Mo La Molybdenum Foils,High Temperature Molybdenum Foil from Supplier or Manufacturer-Shaanxi Getwick Nonferrous Metals ,

High Boiling Point Flat Bottom Molybdenum Boat For

High Boiling Point Flat Bottom Molybdenum Boat For Evaporation Coating , Find Complete Details about High Boiling Point Flat Bottom Molybdenum Boat For Evaporation Coating,Flat Bottom Molybdenum Boat,Molybdenum Boats,Molybdenum Box Boat from Supplier or Manufacturer-Baoji Chengyi Nonferrous Metals ,

Buy Molybdenum Online Advent Research Materials

Molybdenum is an extremely hard metal, making it a useful alloying agent in the It is one of the refractory metals which have very high melting points. Foil, sheet, plate, wire, mesh, tube and rod are available in various sizes and quantities.

Molybdenum Foil online catalogue source supplier of

Buy Molybdenum Foil on-line Rod, Sheet, Single Crystal, Sputtering Target, Tube, Washer, Wire Molybdenum has a high melting point and applications for the pure metal take advantage of this; for example, the pure material is used as

Molybdenum Alloy Plates, Sheets Rods Supplier Eagle

Choose Eagle Alloys as your supplier of Molybdenum alloy plates, sheets, rods, If you do not see your size listed below please our courteous sales Molybdenum is used for its extremely high melting point and relative flexibility.

Molybdenum Plate Products All Sizes Moly Plate made in

Elmet offers high quality % pure molybdenum plate in standard plate thicknesses and with over $30 Million in recent Buy Online For example, its high melting point, 2620 °C, drives its performance in high temperature environments.

Molybdenum sheets / plates|. Corp.

We also offer molybdenum plates with our rolling know-how. Easier to be processed than tungsten and being a high melting point metal, these plates are widely

Molybdenum Supplier Sheet, Plate, Wire, Tubes, Rods

Rembar has molybdenum wires, sheets, rods, tubing, and plates in stock and ready to ship. Access technical These sizes are in stock, subject to prior sale. We also . Pure moly has a very high melting point [2622 °C (4752 °F)]. Only four

Molybdenum Plansee

Because molybdenum possesses a very high melting point, a low coefficient of thermal When used as a base plate, molybdenum reliably dissipates heat.

Molybdenum Sheets in Mumbai, ?????????? ???

Density greater then: /cm3 We are the professional supplier of molybdenum sheets, molybdenum plates, molybdenum discs and sintered molybdenum

Molybdenum Plate AMERICAN ELEMENTS ?

Molybdenum Plate Mo bulk research qty manufacturer. It has the third highest melting point of any element, exceeded only by tungsten and tantalum.

Molybdenum Refractory Metal Rod, Bar, Plate Sheet

Molybdenum is available in Rod, Bar, Plate Sheet Stock. Molybdenum (Mo) has a high melting point and is easy to machine.