• [wzg:title/]
Hastelloy C 276 Electrode For Flowmeter
Hastelloy electrodes for magnetic flow meter. The electrodes widely used for electromagnetic flow meter producing, we can customized according your requirements. 316L electrode , Titanium electrode ,Tantalum electrode ,Hastelloy-C electrode.
Read More
Hastelloy C22 Pipe fittings
Hastelloy C 22 Pipe fittings ( Short Radius Elbows , Long Radius Elbows , Concentric Reducers , Eccentric Reducers , Stub Ends , End Caps , Equal Tees , Weldolets , Pipe Nipples .) ASME/ANSI B16.9, ASME B16.28, MSS-SP-43, MSS SP-79 , Type Seamless / Welded / Fabricated . Hastelloy C-22 / UNS N06022 / DIN W. Nr. 2.4602
Read More
Hastelloy C 276 Pipe fittings
Hastelloy C 276 Pipe fittings ( Short Radius Elbows , Long Radius Elbows , Concentric Reducers , Eccentric Reducers , Stub Ends , End Caps , Equal Tees , Weldolets , Pipe Nipples .) ASME/ANSI B16.9, ASME B16.28, MSS-SP-43, MSS SP-79 , Type Seamless / Welded / Fabricated Hastelloy C276 Pipe Fittings UNS (N10276), DIN (2.4819).
Read More
Inconel 625 Rod
Inconel Round Bar , ASTM B446 Inconel, 625 Bright Round Rod , Inconel 625 Hex Rods ,Inconel 625 flat bar with standard ASTM B446 / ASME SB446 and Nickel Alloy 625/ Inconel 625 (AMS 5666)
Read More
Inconel 601 Welding Wire
Inconel 601 Welding Wire - UNS N06601 - DIN W. Nr.2.4851 . ERNiCrFe-11 (Alloy 601) . ASME II, Part C, SFA-5.14, ERNiCrFe-11 (UNS N06601) , ASME IX, F-No.43 , BS290] NA 49 , DIN 1736 SG-NiCr23Al (2.4626) , (EN) ISO 18274 - SN16601 (NiCr23Fel5Al) , ASME III (NCA3800, NB2400), AMS and other specifications
Read More
Inconel 600 Welding Wire
Inconel 600 Wire ASTM B166 , Inconel 600 welding wire Alloy 600. UNS N06600 / W.Nr. 2.4816 .Nickel Alloy (AWS A5.11) ENiCrFe-3 Welding Electrode, Nickel Alloy ENiCrFe-3 Welding Electrode, ENiCrFe-3 inconel 600
Read More
Invar 32 Wire
Invar 32 Wire Super-Invar 32-5 rod UNS-K-93500, Consisting of 32% Nickel, 5% Cobalt, and the balance Iron, this alloy exhibits minimum thermal expansion (one half of Invar 36) at room temperature. It is often used in structural components, supports and substrates requiring precision measurements. ASTM F1684.
Read More
Invar 32 Sheet
Invar 32 Sheet, plate , Invar Alloy Foil , Super Invar 32-5 Alloy DESCRIPTION. A low expansion alloy consisting of 32% Nickel, 5% Cobalt, balance Iron. This alloy exhibits minimum thermal expansion (one half of Invar 36) Invar-36, Invar-42, Pernifer 36, Invar Steel, Super Invar 32-5, Carpenter 36, 4J32, 4J36
Read More
Invar 36 Plate
Alloy 36 Sheet (Invar) / K93603 / ASTM F1684 Widely known under several trades names such as Invar and Nilo 36**, this grade is a 36% nickel-iron alloy. AMS l-23011 CL7MIL l-23011 CL7UNS K93602/03 4J36 (China), Fe-Ni36 (France), 1.3912, Ni36 (Germany), X1NiCrMoCu, N 25-20-7 (UK) Invar 36, UNSK93600 thermostat alloy, UNSK93601 pressure vessel sheet (USA)
Read More
Alloy 46 Wire
Alloy 46 wire : Consisting of 46% nickel and iron balance, 46 Alloy is a controlled expansion alloy used mostly in electronic applications, especially for glass and ceramic seals. Alloy 46 is also known as Pernifer 462, NILO 464, and Glass-Seal 461 , ,Fe46Ni
Read More
Alloy 46 Sheet
Alloy 46: Consisting of 46% nickel and iron balance, 46 Alloy is a controlled expansion alloy used mostly in electronic applications, especially for glass and ceramic seals. Alloy 46 is also known as Pernifer 462, NILO 464, and Glass-Seal 461
Read More
MP35N Thread Bolt Fastener
MP35N Thread Rod , MP35N bolts , MP35N fasteners , UNS R30035 bolts , MP35N Thread Bar, MP35N Specifications: AMS 5844, AMS 5845, AMS7468, ASTM F562, NACE MR0175. MP35N alloys are used in fasteners, springs, non-magnetic assemblies and instrumentation components in medical, marine, oil and gas well, chemical and food processing environments.
Read More

Request a quote

Glass Melting Molybdenum Electrode 02206

Glass melting electrodes Plansee

Molybdenum glass melting electrodes. Glass melting electrodes must withstand extremely high temperatures and aggressive glass melts. Molybdenum from Plansee is the right material for these challenging conditions. Melting point of 2 620 °C (4 748 °F)

Molybdenum Glass Melting Electrodes American Elements

About Molybdenum Glass Melting Electrodes American Elements specializes in producing high purity Molybdenum Electrodes for use in glass -melting applications. Our glass-melting electrodes are available in multiple dimensions and can include oxidation-resistant coatings, custom threading, and other options.

Glass Melting Electrodes from . Starck

Starck’s molybdenum glass melting electrodes (GME) provide the industry with superior quality and the highest product standards for efficient glass melting and electric boosted melting. The high temperature strength and rigidity of molybdenum electrodes, plus the inherent electrical properties of molybdenum, provide maximum operating efficiency.

Molybdenum Electrode, Molybdenum Electrodes Glass Melting

Molybdenum electrode is widely used in daily glass, optical glass, insulation materials, glass fiber, rare earth industry and glass fiber furnace, glass kiln fore-hearth field because of its excellent properties, such as high strength, oxidation resistance under high temperature, long service life and well corrosion resistance.

Molybdenum in Electrodes for Glass Melting

Molybdenum oxidizes at over 400°C temperatures and hence it is susceptible to oxygen. Earlier, glass melting electrodes were installed in the tank which was full of glass melt. This is a hazardous procedure and takes a lot of time. PLANSEE offers SIBOR, an anti-oxidation solution for molybdenum.

Optimization of Molybdenum Electrodes for Glass Melting

resistance of glass melts causes Joule heating in the molten glass. Molybdenum electrodes for glass melting applications are required to have a high melting temperature, high strength, good oxidation resistance, excellent electrical conductivity, and superior creep behavior at elevated temperatures[8].

Melting glass with molybdenum

The molten glass bath protects these molybdenum components from the rapid oxidation that would occur at that temperature in air, so that they provide long and reliable life. Designers use inert cooling gases or water cooling to protect the portion of the electrode outside the glass bath from oxidation.

Molybdenum Glass Melting Electrode Molybdenum News Center

Molybdenum electrode also known as molybdenum glass melting electrode, mainly because molybdenum electrode having good high temperature strength, good corrosion resistance and long service life, and it is often used in glass furnace for daily-used glass, optical glass, insulating glass, glass fiber materials and other glass marital production, so it is often referred to as molybdenum glass electrode.

REACTION PRODUCTS AND CORROSION OF MOLYBDENUM ELECTRODE IN

The precipitation of metals on a molybdenum electrode in glass melt is probably facilitated by the presence of molybdenum compounds on the molybdenum surface. Corrosion increases through the effect of alternating current most in glass melt without additions, and less in melt containing antimony oxides.

Corrosionpedia What is a Glass Melting Electrode

Glass melting electrodes act as a fuel source in a glass melting plant, must withstand high melting and electric boosted melting temperatures, and are widely used in the glass manufacturing industry. Glass melting electrodes primarily consist of molybdenum with small quantities of zirconium oxide (ZrO 2 ) added to enhance the properties of these electrodes.

Glass melting electrodes Plansee

Glass melting electrodes must withstand extremely high temperatures and aggressive glass melts. Molybdenum from Plansee is the right material for these

Optimization of Molybdenum Electrodes for Glass Melting

situation molybdenum will play a significant role in electrical glass melting, since . Hypothesis for the Failure of Molybdenum Electrodes Used in Melting Glass .

Molybdenum in Electrodes for Glass Melting

9 Jan 2013 Glass melting electrodes must be able to tolerate aggressive glass melts and intensely high temperatures.

Molybdenum Products for Glass Melting Electrodes (GMEs)

12 May 2017 Advantages of Molybdenum. The electric glass melting development is predominantly based on the development of electrode materials. Indeed

Melting glass with molybdenum

help to make the glass and glass products used every day. Molys high strength at the high glass melting temperature and using molybdenum electrodes soon.