• [wzg:title/]
Hastelloy C 276 Electrode For Flowmeter
Hastelloy electrodes for magnetic flow meter. The electrodes widely used for electromagnetic flow meter producing, we can customized according your requirements. 316L electrode , Titanium electrode ,Tantalum electrode ,Hastelloy-C electrode.
Read More
Hastelloy C22 Pipe fittings
Hastelloy C 22 Pipe fittings ( Short Radius Elbows , Long Radius Elbows , Concentric Reducers , Eccentric Reducers , Stub Ends , End Caps , Equal Tees , Weldolets , Pipe Nipples .) ASME/ANSI B16.9, ASME B16.28, MSS-SP-43, MSS SP-79 , Type Seamless / Welded / Fabricated . Hastelloy C-22 / UNS N06022 / DIN W. Nr. 2.4602
Read More
Hastelloy C 276 Pipe fittings
Hastelloy C 276 Pipe fittings ( Short Radius Elbows , Long Radius Elbows , Concentric Reducers , Eccentric Reducers , Stub Ends , End Caps , Equal Tees , Weldolets , Pipe Nipples .) ASME/ANSI B16.9, ASME B16.28, MSS-SP-43, MSS SP-79 , Type Seamless / Welded / Fabricated Hastelloy C276 Pipe Fittings UNS (N10276), DIN (2.4819).
Read More
Inconel 625 Rod
Inconel Round Bar , ASTM B446 Inconel, 625 Bright Round Rod , Inconel 625 Hex Rods ,Inconel 625 flat bar with standard ASTM B446 / ASME SB446 and Nickel Alloy 625/ Inconel 625 (AMS 5666)
Read More
Inconel 601 Welding Wire
Inconel 601 Welding Wire - UNS N06601 - DIN W. Nr.2.4851 . ERNiCrFe-11 (Alloy 601) . ASME II, Part C, SFA-5.14, ERNiCrFe-11 (UNS N06601) , ASME IX, F-No.43 , BS290] NA 49 , DIN 1736 SG-NiCr23Al (2.4626) , (EN) ISO 18274 - SN16601 (NiCr23Fel5Al) , ASME III (NCA3800, NB2400), AMS and other specifications
Read More
Inconel 600 Welding Wire
Inconel 600 Wire ASTM B166 , Inconel 600 welding wire Alloy 600. UNS N06600 / W.Nr. 2.4816 .Nickel Alloy (AWS A5.11) ENiCrFe-3 Welding Electrode, Nickel Alloy ENiCrFe-3 Welding Electrode, ENiCrFe-3 inconel 600
Read More
Invar 32 Wire
Invar 32 Wire Super-Invar 32-5 rod UNS-K-93500, Consisting of 32% Nickel, 5% Cobalt, and the balance Iron, this alloy exhibits minimum thermal expansion (one half of Invar 36) at room temperature. It is often used in structural components, supports and substrates requiring precision measurements. ASTM F1684.
Read More
Invar 32 Sheet
Invar 32 Sheet, plate , Invar Alloy Foil , Super Invar 32-5 Alloy DESCRIPTION. A low expansion alloy consisting of 32% Nickel, 5% Cobalt, balance Iron. This alloy exhibits minimum thermal expansion (one half of Invar 36) Invar-36, Invar-42, Pernifer 36, Invar Steel, Super Invar 32-5, Carpenter 36, 4J32, 4J36
Read More
Invar 36 Plate
Alloy 36 Sheet (Invar) / K93603 / ASTM F1684 Widely known under several trades names such as Invar and Nilo 36**, this grade is a 36% nickel-iron alloy. AMS l-23011 CL7MIL l-23011 CL7UNS K93602/03 4J36 (China), Fe-Ni36 (France), 1.3912, Ni36 (Germany), X1NiCrMoCu, N 25-20-7 (UK) Invar 36, UNSK93600 thermostat alloy, UNSK93601 pressure vessel sheet (USA)
Read More
Alloy 46 Wire
Alloy 46 wire : Consisting of 46% nickel and iron balance, 46 Alloy is a controlled expansion alloy used mostly in electronic applications, especially for glass and ceramic seals. Alloy 46 is also known as Pernifer 462, NILO 464, and Glass-Seal 461 , ,Fe46Ni
Read More
Alloy 46 Sheet
Alloy 46: Consisting of 46% nickel and iron balance, 46 Alloy is a controlled expansion alloy used mostly in electronic applications, especially for glass and ceramic seals. Alloy 46 is also known as Pernifer 462, NILO 464, and Glass-Seal 461
Read More
MP35N Thread Bolt Fastener
MP35N Thread Rod , MP35N bolts , MP35N fasteners , UNS R30035 bolts , MP35N Thread Bar, MP35N Specifications: AMS 5844, AMS 5845, AMS7468, ASTM F562, NACE MR0175. MP35N alloys are used in fasteners, springs, non-magnetic assemblies and instrumentation components in medical, marine, oil and gas well, chemical and food processing environments.
Read More

Request a quote

Cold Rolled Mo 1 Molybdenum Sheet For Heating Shield

Molybdenum Sheet

Description: AEM is a leading global provider of high quality molybdenum sheet products. AEM offers a wide range of cold rolled sheet product in varying thickness and length and per customer request. As with all of our materials, our sheet begins as metal powder, is pressed into ingots, sintered, an

Molybdenum Sheet, Molybdenum Sheet Sale Price, Molybdenum

Molybdenum sheet is primarily used as heating shield, heating component, electric light and vacuum component, vacuum electronic device, electronic component, irregular part. Specification: Molybdenum rod is manufactured as random length pieces or cut to customers’ desired lengths in diameters ranging from inches to inches.

Molybdenum sheet and foil Supply Bango Alloy

molybdenum sheet is widely used in reflection shield, cover plate applied in the sapphire growth furnace, reflection shield, heating tape, connecting pieces applied in vacuum furnace, sputtering target applied in plasma coating film, and high temperature resistance boat.

Molybdenum Sheet Stanford Materials

Molybdenum sheet is used for making electric light source parts, components of electric vacuum and electric power semiconductor. It is also used for producing molybdenum boats, heat shield and heat bodies in high temperature furnace. Specification: We produce high quality molybdenum sheet as one of our hot product.

Molybdenum Sheet Products Elmet Technologies

Elmet is a leading global provider of high-quality molybdenum sheet products and the only US owned and operated producer. Elmet offers a wide range of cold rolled sheet product in varying thickness and length and per customer request.

% Pure HotRolled Polished Molybdenum Sheets/Plate for

Molybdenum Sheets, Heating Shield, Mo Sheet /Plate manufacturer / supplier in China, offering % Pure Hot-Rolled Polished Molybdenum Sheets/Plate for Heat Shield with Factory Price, % Pure Tungsten Tubes Tungsten Pipes ASTM B760, Molybdenum Wire for Cutting Dia and so on.

cold rolling molybdenum sheet

offers 908 cold rolling molybdenum sheet products. About 80% of these are molybdenum, 9% are other metals metal products, and 2% are steel sheets. A wide variety of cold rolling molybdenum sheet options are available to you, such as cold rolled, hot rolled, and rolled.

Molybdenum Plate,Molybdenum Heating Tape,Molybdenum

Molybdenum plate and sheet and molybdenum reflection shield are packed in plywood case and sent by ocean or air. Zhuzhou Jiabang Refractory Metal , was founded in 2008, specializing molybdenum products, such as molybdenum plate (molybdenum sheet). With rich experience, our products are in superior quality, gaining widespread recognition.

Molybdenum sheets Plansee

Thanks to our high capacities, we can manufacture even very large quantities of molybdenum sheets without difficulty. Thanks to our state-of-the-art equipment and many years of experience in the field of powder metallurgy, we can guarantee that you receive top quality - in every molybdenum sheet we supply.

Molybdenum Supplier Sheet, Plate, Wire, Tubes, Rods

“Superplastic” deformation during the process produces a near-net-shape forging with greatly reduced machining cost and better mechanical properties compared to traditionally forged parts. Only dies and other components made from molybdenum TZM (% % Zr) and MHC (Mo-1/2% Hf- % C) alloys can withstand this process.

China Bright Cold Rolled Molybdenum Sheet Thickness

Bright Cold Rolled Molybdenum Sheet Thickness mm Used in Heating Shield . Mo-1. Density. More Than /Cc. Trademark. HP. Transport Package.

Molybdenum Mo Sheet

1348 products China Molybdenum Mo Sheet manufacturers - Select 2019 high quality Molybdenum Mo Polishing Molybdenum Sheet Mo1 Mola Sheet . Hot Sale Mo85cu Molybdenum Copper Alloy Sheet for Heating Element Sintered % Cold Rolled Molybdenum Sheets (with lanthanum) in High Grade Mo-1.

Molybdenum Sheet Stanford Materials

It is also used for producing molybdenum boats, heat shield and heat bodies in high We produce high quality molybdenum sheet as one of our hot product. Molybdenum flat products are rolled and annealed to provide the optimum condition Mo-1. Mo-2. Mo-3. Mo(%). . . . Other Element Content(%) ≤.

China High Quality Molybdenum Sheets Suppliers

1. Molybdenum sheets are used for producing molybdenum electrodes, heating elements, heat shields, sintering trays, sintering boats, stacking sheets, base sheetss, Owning two hot rolling machine and five cold rolling machines, We can Mo-La sheet, tungsten and molybdenum sheets, tungsten and molybdenum discs

Molybdenum sheet Molybdenum product Tungsten alloy

1 Physical and chemical properties. 1. Mo billet. 2 Measurements of sheet billet Hot rolled. Hot mill. 1 Measurements (thickness, width). 4. Annealing Molybdenum sheet is widely used in reflection shield, cover plate applied in the sapphire

Molybdenum Plansee

CFDEM modelling of particle heating and acceleration in cold spraying definitely because of the production process (multiple heat treatment at temperatures above 1 000 °C in H2-atmosphere) When used as a base plate, molybdenum reliably dissipates heat. .. Typical tensile strength for Mo and TZM sheet material in

Applications of Molybdenum Metal and Its Alloys

Page 1 Prepared by John A. Shields, Jr., . Hot rolling molybdenum creates spectacular heat and smoke. Figure 1. Flowsheet describing the production of molybdenum metal mill products. oxide, contains about 57% Mo and less.

High Temperature Alloys for Furnace Applications AZoM

12 May 2017 Alloys of molybdenum, niobium, tantalum, and tungsten such as MoLa and fixtures, and fabricates components such as heat shields, furnace racks, hot zones, boats Mo 75wt% and W 25wt% alloy to serve as heat shields in furnaces. pure tungsten metal powder into an ingot for hot, and cold rolling.

China MOLYBDENUM SHEET Manufacturers Suppliers

30 products Getwick offers a wide range of cold rolled sheet product in varying thickness and length TZM Molybdenum Sheet Price per KG for Heating Shield.

Tungsten Sheet Products All Sheet Sizes Tungsten Sheet

Elmet offers a wide range of hot rolled tungsten plate and cold rolled tungsten sheet boats, as components in high-temperature furnaces and as heat shields.

  • share:

Request a quote