• [wzg:title/]
Hastelloy C 276 Electrode For Flowmeter
Hastelloy electrodes for magnetic flow meter. The electrodes widely used for electromagnetic flow meter producing, we can customized according your requirements. 316L electrode , Titanium electrode ,Tantalum electrode ,Hastelloy-C electrode.
Read More
Hastelloy C22 Pipe fittings
Hastelloy C 22 Pipe fittings ( Short Radius Elbows , Long Radius Elbows , Concentric Reducers , Eccentric Reducers , Stub Ends , End Caps , Equal Tees , Weldolets , Pipe Nipples .) ASME/ANSI B16.9, ASME B16.28, MSS-SP-43, MSS SP-79 , Type Seamless / Welded / Fabricated . Hastelloy C-22 / UNS N06022 / DIN W. Nr. 2.4602
Read More
Hastelloy C 276 Pipe fittings
Hastelloy C 276 Pipe fittings ( Short Radius Elbows , Long Radius Elbows , Concentric Reducers , Eccentric Reducers , Stub Ends , End Caps , Equal Tees , Weldolets , Pipe Nipples .) ASME/ANSI B16.9, ASME B16.28, MSS-SP-43, MSS SP-79 , Type Seamless / Welded / Fabricated Hastelloy C276 Pipe Fittings UNS (N10276), DIN (2.4819).
Read More
Inconel 625 Rod
Inconel Round Bar , ASTM B446 Inconel, 625 Bright Round Rod , Inconel 625 Hex Rods ,Inconel 625 flat bar with standard ASTM B446 / ASME SB446 and Nickel Alloy 625/ Inconel 625 (AMS 5666)
Read More
Inconel 601 Welding Wire
Inconel 601 Welding Wire - UNS N06601 - DIN W. Nr.2.4851 . ERNiCrFe-11 (Alloy 601) . ASME II, Part C, SFA-5.14, ERNiCrFe-11 (UNS N06601) , ASME IX, F-No.43 , BS290] NA 49 , DIN 1736 SG-NiCr23Al (2.4626) , (EN) ISO 18274 - SN16601 (NiCr23Fel5Al) , ASME III (NCA3800, NB2400), AMS and other specifications
Read More
Inconel 600 Welding Wire
Inconel 600 Wire ASTM B166 , Inconel 600 welding wire Alloy 600. UNS N06600 / W.Nr. 2.4816 .Nickel Alloy (AWS A5.11) ENiCrFe-3 Welding Electrode, Nickel Alloy ENiCrFe-3 Welding Electrode, ENiCrFe-3 inconel 600
Read More
Invar 32 Wire
Invar 32 Wire Super-Invar 32-5 rod UNS-K-93500, Consisting of 32% Nickel, 5% Cobalt, and the balance Iron, this alloy exhibits minimum thermal expansion (one half of Invar 36) at room temperature. It is often used in structural components, supports and substrates requiring precision measurements. ASTM F1684.
Read More
Invar 32 Sheet
Invar 32 Sheet, plate , Invar Alloy Foil , Super Invar 32-5 Alloy DESCRIPTION. A low expansion alloy consisting of 32% Nickel, 5% Cobalt, balance Iron. This alloy exhibits minimum thermal expansion (one half of Invar 36) Invar-36, Invar-42, Pernifer 36, Invar Steel, Super Invar 32-5, Carpenter 36, 4J32, 4J36
Read More
Invar 36 Plate
Alloy 36 Sheet (Invar) / K93603 / ASTM F1684 Widely known under several trades names such as Invar and Nilo 36**, this grade is a 36% nickel-iron alloy. AMS l-23011 CL7MIL l-23011 CL7UNS K93602/03 4J36 (China), Fe-Ni36 (France), 1.3912, Ni36 (Germany), X1NiCrMoCu, N 25-20-7 (UK) Invar 36, UNSK93600 thermostat alloy, UNSK93601 pressure vessel sheet (USA)
Read More
Alloy 46 Wire
Alloy 46 wire : Consisting of 46% nickel and iron balance, 46 Alloy is a controlled expansion alloy used mostly in electronic applications, especially for glass and ceramic seals. Alloy 46 is also known as Pernifer 462, NILO 464, and Glass-Seal 461 , ,Fe46Ni
Read More
Alloy 46 Sheet
Alloy 46: Consisting of 46% nickel and iron balance, 46 Alloy is a controlled expansion alloy used mostly in electronic applications, especially for glass and ceramic seals. Alloy 46 is also known as Pernifer 462, NILO 464, and Glass-Seal 461
Read More
MP35N Thread Bolt Fastener
MP35N Thread Rod , MP35N bolts , MP35N fasteners , UNS R30035 bolts , MP35N Thread Bar, MP35N Specifications: AMS 5844, AMS 5845, AMS7468, ASTM F562, NACE MR0175. MP35N alloys are used in fasteners, springs, non-magnetic assemblies and instrumentation components in medical, marine, oil and gas well, chemical and food processing environments.
Read More

Request a quote

Ceramic Heater Mosi2 Molybdenum Disilicideheating Elements

MoSi2 Heating Elements Sentro Tech

MoSi2 Heating Element Products. Specifically made for industrial and laboratory furnaces, the MoSi2 heating elements are a ceramic based resistant element that can produce furnace temperature to 1800°C. These custom heating elements are known for their longevity and reliability at a high temperature.

Molybdenum Disilicide Mosi2 heating elements Silcarb

MoSi2 heating elements are supplied as ready-made elements and are produced as either straight, bent forms or multi shank elements and in a wide range of dimensions. The elements are used mainly in laboratory furnaces and production furnaces in the glass, electronics, steel, ceramics, and heat treatment industries.

Kanthal Super MoSi2 heating elements — Kanthal?

High-power electric molybdenum disilicide (MoSi2) heating elements for element temperatures up to 1850°C (3360°F). Kanthal Super MoSi2 heating elements are available as straight or bent elements in a wide range of shapes and sizes.

MolyCom? – Intermetallic molybdenum disilicide heating

The electrical heating elements with the brand names MolyCom? consist of intermetallic molybdenum disilicide (MoSi2) and ceramic additives.

MOSi2 Heating Element

Molybdenum disilicide (MoSi2) heating element is a resistance generate-heating component made from MoSi2 or the basic material. It is used in high temperature under the oxidizing atmosphere, it looks like glass in its surface and form a light SiO2 glass film which can protect the element not to be oxidized.

Molybdenum Disilicide Heating Element MoSi2

MP? Class: Conventional U-shaped MP class Molybdenum disilicide elements may be heated to 1900°C. The MP1800 type elements are more commonly used and are able to achieve 1830°C. The MP1800 type elements are more commonly used and are able to achieve 1830°C.

MoSi2 Heating Element Unison Commercial Inc.

MoSi2 Heating Element High-power electric molybdenum disilicide (MoSi2) heating elements for element temperatures up to 1850°C (3360°F). Kanthal Super MoSi2 heating elements are available as straight or bent elements in a wide range of shapes and sizes, all characterized by long life and consistent performance.

MoSiO2 Elements (MolyD or Molybdenum Disilicide) Keith Company

MoSi2 elements also offer the longest inherent life of all electric heating elements. Molybdenum disilicide elements are manufactured in several grades of elements, with the primary difference being the MET in a certain atmosphere.

MolyD Molybdenum Disilicide Mosi2 Heating Elements

Moly-D Molybdenum Disilicide Mosi2 Heating Elements Description: Molybdenum disilicide (MoSi2) heating element is a resistance generate-heating component made from MoSi2 or the basic material. It is used in high temperature under the oxidizing atmosphere. So this kind of element has unique effect for resisting oxidization in the high temperature.

Molybdenum disilicide (MoSi2 Electric heating elements and

Molybdenum disilicide (MoSi2) are resistance type heating elements made of a dense ceramic-metallic material which can produce furnace temperatures approaching 1800°C. Although more expensive than traditional metallic elements, MoSi2 elements are known for their longevity due

MoSi2 Heating Element Molybdenum di silicide Element

Molybdenum Disilicide Ceramic Mosi2 Heating Element Power Strap Rs 470/ Kilogram MoSi2 Heating Element ( Molybdenum Disilicide Heating Element ).

Kanthal Super MoSi2 heating elements — Kanthal?

High-power electric molybdenum disilicide (MoSi2) heating elements for element temperatures up to 1850°C (3360°F). Kanthal Super MoSi2 heating elements

Intermetallic molybdenum disilicide heating elements (MoSi2)

16 Mar 2016 Intermetallic molybdenum disilicide heating elements (MoSi2) at SCHUPP? Ceramics makes high temperature technology to suit your

Molybdenum Disilicide Mosi2 heating elements Silcarb

Molybdenum Disilicide Heating Elements Molybdenum Di Silicide (MoSi2) is a special material that has the best properties of both ceramic and metallic

MoSi2 Heating Element National Enterprise, Mumbai

Manufacturer of MoSi2 Heating Element - MoSi2 Heating Element ( Molybdenum Disilicide Heating Element ) offered by National Enterprise, Mumbai,

MoSiO2 Elements (MolyD or Molybdenum Disilicide) Keith

MoSiO2 (MolyD or Molybdenum Disilicide) heating elements Molybdenum disilicide (MoSi2) elements are available in a variety of shapes and sizes MoSi2 elements also offer the longest inherent life of all electric heating elements . Most expensive of the elements under consideration; Ceramic material risk of fracture.

Molybdenum disilicide

Molybdenum disilicide an intermetallic compound, a silicide of molybdenum, is a refractory ceramic with primary use in heating elements. MoSi2 is a gray metallic-looking material with tetragonal crystal structure (alpha-modification); Molybdenum disilicide heating elements can be used for temperatures up to 1800 °C,

MolyD Molybdenum Disilicide MoSi2 Heating Elements On I

Browse Moly-D Molybdenum Disilicide MoSi2 Heating Elements in the I Squared R Element , Inc. catalog including Moly-D Molybdenum Disilicide Heating Elements,Moly-D Molybdenum Disilicide Heating Element Ceramic Holder

Molybdenum Disilicide Heating Elements Berghütten

Molybdenum Disilicide Heating Elements consisting of Molybd?n-Disilizid ( MoSi2) with ceramic additives.

MoSi2 Heating Elements for High Temperature Furnaces

A ceramic-based resistant element, the MoSi2 heating elements produce furnace temperature Molybdenum Disilicide Heating Elements Temperature Grades.