• [wzg:title/]
Hastelloy C 276 Electrode For Flowmeter
Hastelloy electrodes for magnetic flow meter. The electrodes widely used for electromagnetic flow meter producing, we can customized according your requirements. 316L electrode , Titanium electrode ,Tantalum electrode ,Hastelloy-C electrode.
Read More
Hastelloy C22 Pipe fittings
Hastelloy C 22 Pipe fittings ( Short Radius Elbows , Long Radius Elbows , Concentric Reducers , Eccentric Reducers , Stub Ends , End Caps , Equal Tees , Weldolets , Pipe Nipples .) ASME/ANSI B16.9, ASME B16.28, MSS-SP-43, MSS SP-79 , Type Seamless / Welded / Fabricated . Hastelloy C-22 / UNS N06022 / DIN W. Nr. 2.4602
Read More
Hastelloy C 276 Pipe fittings
Hastelloy C 276 Pipe fittings ( Short Radius Elbows , Long Radius Elbows , Concentric Reducers , Eccentric Reducers , Stub Ends , End Caps , Equal Tees , Weldolets , Pipe Nipples .) ASME/ANSI B16.9, ASME B16.28, MSS-SP-43, MSS SP-79 , Type Seamless / Welded / Fabricated Hastelloy C276 Pipe Fittings UNS (N10276), DIN (2.4819).
Read More
Inconel 625 Rod
Inconel Round Bar , ASTM B446 Inconel, 625 Bright Round Rod , Inconel 625 Hex Rods ,Inconel 625 flat bar with standard ASTM B446 / ASME SB446 and Nickel Alloy 625/ Inconel 625 (AMS 5666)
Read More
Inconel 601 Welding Wire
Inconel 601 Welding Wire - UNS N06601 - DIN W. Nr.2.4851 . ERNiCrFe-11 (Alloy 601) . ASME II, Part C, SFA-5.14, ERNiCrFe-11 (UNS N06601) , ASME IX, F-No.43 , BS290] NA 49 , DIN 1736 SG-NiCr23Al (2.4626) , (EN) ISO 18274 - SN16601 (NiCr23Fel5Al) , ASME III (NCA3800, NB2400), AMS and other specifications
Read More
Inconel 600 Welding Wire
Inconel 600 Wire ASTM B166 , Inconel 600 welding wire Alloy 600. UNS N06600 / W.Nr. 2.4816 .Nickel Alloy (AWS A5.11) ENiCrFe-3 Welding Electrode, Nickel Alloy ENiCrFe-3 Welding Electrode, ENiCrFe-3 inconel 600
Read More
Invar 32 Wire
Invar 32 Wire Super-Invar 32-5 rod UNS-K-93500, Consisting of 32% Nickel, 5% Cobalt, and the balance Iron, this alloy exhibits minimum thermal expansion (one half of Invar 36) at room temperature. It is often used in structural components, supports and substrates requiring precision measurements. ASTM F1684.
Read More
Invar 32 Sheet
Invar 32 Sheet, plate , Invar Alloy Foil , Super Invar 32-5 Alloy DESCRIPTION. A low expansion alloy consisting of 32% Nickel, 5% Cobalt, balance Iron. This alloy exhibits minimum thermal expansion (one half of Invar 36) Invar-36, Invar-42, Pernifer 36, Invar Steel, Super Invar 32-5, Carpenter 36, 4J32, 4J36
Read More
Invar 36 Plate
Alloy 36 Sheet (Invar) / K93603 / ASTM F1684 Widely known under several trades names such as Invar and Nilo 36**, this grade is a 36% nickel-iron alloy. AMS l-23011 CL7MIL l-23011 CL7UNS K93602/03 4J36 (China), Fe-Ni36 (France), 1.3912, Ni36 (Germany), X1NiCrMoCu, N 25-20-7 (UK) Invar 36, UNSK93600 thermostat alloy, UNSK93601 pressure vessel sheet (USA)
Read More
Alloy 46 Wire
Alloy 46 wire : Consisting of 46% nickel and iron balance, 46 Alloy is a controlled expansion alloy used mostly in electronic applications, especially for glass and ceramic seals. Alloy 46 is also known as Pernifer 462, NILO 464, and Glass-Seal 461 , ,Fe46Ni
Read More
Alloy 46 Sheet
Alloy 46: Consisting of 46% nickel and iron balance, 46 Alloy is a controlled expansion alloy used mostly in electronic applications, especially for glass and ceramic seals. Alloy 46 is also known as Pernifer 462, NILO 464, and Glass-Seal 461
Read More
MP35N Thread Bolt Fastener
MP35N Thread Rod , MP35N bolts , MP35N fasteners , UNS R30035 bolts , MP35N Thread Bar, MP35N Specifications: AMS 5844, AMS 5845, AMS7468, ASTM F562, NACE MR0175. MP35N alloys are used in fasteners, springs, non-magnetic assemblies and instrumentation components in medical, marine, oil and gas well, chemical and food processing environments.
Read More

Request a quote

B423 N08825 Incoloy 825 Nickel Iron Chromium Molybdenum Copper Alloy Seamless Pipe And Tube

ASTM B423 Incoloy Alloy 825 Seamless Pipe Tube · ASTM B423

ASTM B423 specification covers Inconel 825 (UNS N08825)in the form of cold-worked and hot-finished seamless pipe and tube intended for general corrosive service. ASTM B423 - Seamless Pipe and Tube ASTM B423 Seamless Tube is a nickel-iron-chromium alloy with additions of copper, molybdenum and titanium.

Incoloy 825 N08825 Nickel Alloy Tubing ASTM B163 B423 ASME

ASTM B163 B423 ASME SB163 SB423 N08825 Nickel Alloy Seamless Tubes Tubing Pipes is a nickel-iron-chromium alloy with additions of molybdenum and copper. This nickel steel alloy’s chemical composition is designed to provide exceptional resistance to many corrosive environments.

Standard Specification for NickelIronChromiumMolybdenum

This specification covers nickel-iron-chromium-molybdenum-copper alloys (UNS N08825 and UNS N08221) in the form of cold-worked and hot-finished seamless pipe and tube intended for general corrosive service. Material furnished under this specification shall conform to the applicable requirements specified.

Inconel 825 Tubes, Incoloy 825 ASTM B423 Seamless Tubes

Incoloy alloy 825 is a nickel-iron-chromium alloy with additions of copper, molybdenum and titanium. The alloys chemical composition is designed to provide exceptional resistance to many corrosive environments. The nickel content is sufficient for resistance to chloride-ion stress corrosion cracking.

ASTM B423 Seamless Pipe and Tube

ASTM B423 specification covers nickel-iron-chromium-molybdenum-copper alloys (UNS N08825) in the form of cold-worked and hot-finished seamless pipe and tube intended for general corrosive service. Material furnished under this specification shall conform to the applicable requirements specified.

ASTM B423 INCOLOY 825 SEAMLESS PIPES

INCOLOY 825 SEAMLESS Pipes Incoloy 825 is a nickel-iron-chromium alloy with additions of molybdenum and copper. This nickel steel alloys chemical composition is designed to provide exceptional resistance to many corrosive environments.

Standard Specification for NickelIronChromiumMolybdenum

This specification covers nickel-iron-chromium-molybdenum-copper alloys (UNS N08825, N08221, and N06845) in the form of cold-worked and hot-finished seamless pipe and tube intended for general corrosive service. The general requirements for pipe and tube are covered in Specification B829.

Incoloy 825 Alloy 825 UNS N08825 MEGA MEX

Incoloy 825 is a nickel-iron-chromium alloy with additions of molybdenum, copper and titanium. This nickel steel alloy’s chemical composition is designed to provide exceptional resistance to many corrosive environments. It is similar to alloy 800 but has improved resistance to aqueous corrosion.

Incoloy 825 Tubing ALLOY METALS AND TUBES INTERNATIONAL

Incoloy? Alloy 825 (UNS N08825/. ) is a nickel-iron-chromium alloy with additions of copper, molybdenum and titanium.

Alloy 825 Premium Nickel Alloys from NeoNickel

A nickel-iron-chromium grade with addition of molybdenum and copper, Alloy 825 has excellent corrosion resistance. Alloy 825 is a high performing nickel-iron-chromium alloy with additions of molybdenum, copper, and titanium. The nickel content is sufficient for resistance to chloride-ion stress-corrosion cracking.

ASTM B423 Incoloy Alloy 825 Seamless Pipe Tube · ASTM

ASTM B423 specification covers nickel-iron-chromium-molybdenum-copper alloys (UNS N08825) in the form of cold-worked and hot-finished seamless pipe

ASTM B423 Seamless Pipe and Tube Ganpat Industrial

13 Apr 2019 ASTM B423 Nickel-Iron-Chromium Alloys Seamless Tubes, Inconel 825 Pipes, Incoloy N08825 Pipe, ASTM B423 Incoloy Seamless Pipe, ASME SB 423 Nickel-Iron-Chromium-Molybdenum-Copper Alloy Seamless Tubes

Inconel 825 Tubes, Incoloy 825 ASTM B423 Seamless Tubes

Inconel 825 ASTM B423/ ASME B423 Tubes (UNS N08825) Incoloy alloy 825 is a nickel-iron-chromium alloy with additions of copper, molybdenum and titanium. The molybdenum also aids resistance to pitting and crevice corrosion.

Incoloy 825 Alloy 825 UNS N08825 MEGA MEX

Incoloy 825 (UNS N08825), a corrosion resistant nickel alloy, is supplied by Mega Mex in various forms. Incoloy 825 is a nickel-iron-chromium alloy with additions of molybdenum, copper and titanium. Sheet; Plate; Bar; Pipe Fittings (. flanges, slip-ons, blinds, weld-necks, lapjoints, long

ASTM B423 UNS N08825(Incoloy 825) Nickel Alloy Tube

24 Nov 2018 ASTM B423 Standard Specification for Nickel-Iron-Chromium-Molybdenum- Copper Alloy (UNS N08825 and N08221)* Seamless Pipe and

Nickel Alloy 825 Datasheet Fine Tubes

Technical information on Nickel Alloy 825 ? UNS N08825 ? Werkstoff Nr. . austenitic nickel-iron-chromium alloy with additions of molybdenum, copper

Specification of Incoloy 825 UNS N08825 Seamless Tubes

Tubes ASTM B-423. Nickel-Iron-Chromium-Molybdenum-Copper Alloy (UNS N08825 and N08221) Seamless Pipe and Tube ASTM E-571. Electromagnetic

Incoloy 825 N08825 Nickel Alloy Tubing ASTM B163 B423

B423 ASME SB163 SB423 N08825 Nickel Alloy Seamless Tubes Tubing Pipes in is a nickel-iron-chromium alloy with additions of molybdenum and copper.

Alloy 825 Seamless Pressure Tubing Prysmian Group

Description. Alloy 825 is a titanium-stabilized austenitic nickel - iron - chromium ASTM B423, Standard Specification for Nickel-Iron-Chromium—. Molybdenum- Copper Alloy (UNS N08825 and N08221) Seamless. Pipe and Tube. Meets the

Hart bv, Stockholder of Nickel Alloy Piping Products

Nickel 200 201 Monel 400 K500 Inconel 600 601 625 825 Alloy Pipes Flanges Fittings Pipe (seamless and welded in random lengths and cut to size); Fittings (BW and forged fittings) UNS N08825 is a nickel-iron-chromium alloy with molybdenum and copper added to it. Welded Tubing - B704 Seamless Pipe - B423