• [wzg:title/]
Hastelloy C 276 Electrode For Flowmeter
Hastelloy electrodes for magnetic flow meter. The electrodes widely used for electromagnetic flow meter producing, we can customized according your requirements. 316L electrode , Titanium electrode ,Tantalum electrode ,Hastelloy-C electrode.
Read More
Hastelloy C22 Pipe fittings
Hastelloy C 22 Pipe fittings ( Short Radius Elbows , Long Radius Elbows , Concentric Reducers , Eccentric Reducers , Stub Ends , End Caps , Equal Tees , Weldolets , Pipe Nipples .) ASME/ANSI B16.9, ASME B16.28, MSS-SP-43, MSS SP-79 , Type Seamless / Welded / Fabricated . Hastelloy C-22 / UNS N06022 / DIN W. Nr. 2.4602
Read More
Hastelloy C 276 Pipe fittings
Hastelloy C 276 Pipe fittings ( Short Radius Elbows , Long Radius Elbows , Concentric Reducers , Eccentric Reducers , Stub Ends , End Caps , Equal Tees , Weldolets , Pipe Nipples .) ASME/ANSI B16.9, ASME B16.28, MSS-SP-43, MSS SP-79 , Type Seamless / Welded / Fabricated Hastelloy C276 Pipe Fittings UNS (N10276), DIN (2.4819).
Read More
Inconel 625 Rod
Inconel Round Bar , ASTM B446 Inconel, 625 Bright Round Rod , Inconel 625 Hex Rods ,Inconel 625 flat bar with standard ASTM B446 / ASME SB446 and Nickel Alloy 625/ Inconel 625 (AMS 5666)
Read More
Inconel 601 Welding Wire
Inconel 601 Welding Wire - UNS N06601 - DIN W. Nr.2.4851 . ERNiCrFe-11 (Alloy 601) . ASME II, Part C, SFA-5.14, ERNiCrFe-11 (UNS N06601) , ASME IX, F-No.43 , BS290] NA 49 , DIN 1736 SG-NiCr23Al (2.4626) , (EN) ISO 18274 - SN16601 (NiCr23Fel5Al) , ASME III (NCA3800, NB2400), AMS and other specifications
Read More
Inconel 600 Welding Wire
Inconel 600 Wire ASTM B166 , Inconel 600 welding wire Alloy 600. UNS N06600 / W.Nr. 2.4816 .Nickel Alloy (AWS A5.11) ENiCrFe-3 Welding Electrode, Nickel Alloy ENiCrFe-3 Welding Electrode, ENiCrFe-3 inconel 600
Read More
Invar 32 Wire
Invar 32 Wire Super-Invar 32-5 rod UNS-K-93500, Consisting of 32% Nickel, 5% Cobalt, and the balance Iron, this alloy exhibits minimum thermal expansion (one half of Invar 36) at room temperature. It is often used in structural components, supports and substrates requiring precision measurements. ASTM F1684.
Read More
Invar 32 Sheet
Invar 32 Sheet, plate , Invar Alloy Foil , Super Invar 32-5 Alloy DESCRIPTION. A low expansion alloy consisting of 32% Nickel, 5% Cobalt, balance Iron. This alloy exhibits minimum thermal expansion (one half of Invar 36) Invar-36, Invar-42, Pernifer 36, Invar Steel, Super Invar 32-5, Carpenter 36, 4J32, 4J36
Read More
Invar 36 Plate
Alloy 36 Sheet (Invar) / K93603 / ASTM F1684 Widely known under several trades names such as Invar and Nilo 36**, this grade is a 36% nickel-iron alloy. AMS l-23011 CL7MIL l-23011 CL7UNS K93602/03 4J36 (China), Fe-Ni36 (France), 1.3912, Ni36 (Germany), X1NiCrMoCu, N 25-20-7 (UK) Invar 36, UNSK93600 thermostat alloy, UNSK93601 pressure vessel sheet (USA)
Read More
Alloy 46 Wire
Alloy 46 wire : Consisting of 46% nickel and iron balance, 46 Alloy is a controlled expansion alloy used mostly in electronic applications, especially for glass and ceramic seals. Alloy 46 is also known as Pernifer 462, NILO 464, and Glass-Seal 461 , ,Fe46Ni
Read More
Alloy 46 Sheet
Alloy 46: Consisting of 46% nickel and iron balance, 46 Alloy is a controlled expansion alloy used mostly in electronic applications, especially for glass and ceramic seals. Alloy 46 is also known as Pernifer 462, NILO 464, and Glass-Seal 461
Read More
MP35N Thread Bolt Fastener
MP35N Thread Rod , MP35N bolts , MP35N fasteners , UNS R30035 bolts , MP35N Thread Bar, MP35N Specifications: AMS 5844, AMS 5845, AMS7468, ASTM F562, NACE MR0175. MP35N alloys are used in fasteners, springs, non-magnetic assemblies and instrumentation components in medical, marine, oil and gas well, chemical and food processing environments.
Read More

Request a quote

165mesh Molybdenum Wire Mesh

Molybdenum Wire Mesh Manufacturer&Supplier Deze Wire

Molybdenum wire mesh made by pure molybdenum or molybdenum yttrium. Surface of the Molybdenum wire mesh: Bright pure molybdenum wire molybdenum content ≥ %; Black pure molybdenum wire (graphite coating on the surface); Molybdenum yttrium alloy %; yttrium content %; Mesh hole shape: square. Melting point: 2610°C. Aperture: 0

Molybdenum Wire Mesh for Sieving and Filtering

Molybdenum Wire Mesh is a type of woven wire mesh, which is made of pure molybdenum wires or alloy wires. According to the weaving patterns, molybdenum wire mesh has plain weave, twill weave, dutch weave patterns with square and rectangular shaped holes on surface.

Thermo Shield Molybdenum Screen

Molybdenum refractory screen is known under many names (Mesh, Wire Cloth, Screen Grid, Wire Mesh). It has a high strength to weight ratio, is not subject to hydrogen embrittlement, is more ductile than tungsten and only one half as dense.

Molybdenum Wire Mesh, Molybdenum Mesh

Molybdenum Mesh is made with Molybdenum wire. It has very similar properties with tungsten in many conditions. Molybdenum has very high melting point about 2,623oC or 4,753oF and it can withstand extremely high pressure and temperature conditions without changing its structure noticeably.

Molybdenum (Moly) Wire Cloth Belleville Wire Cloth , Inc.

Browse Molybdenum (Moly) Wire Cloth in the Belleville Wire Cloth , Inc. catalog including Item #,Mesh(per lineal inch),Wire Diameter,Width of Opening,Open Area,Price per Square Foot(Volume Disc.

Molybdenum Mesh Wire Mesh Screens for Industrial

Molybdenum Mesh; Monel Mesh; Brass Mesh; Phosphor Bronze Mesh; Hastealloy Mesh; Incoloy Mesh; Fabricated wire mesh; Mosquito fly mesh; Chicken mesh; Chain link

Molybdenum gauze, 165 mesh woven from (0

Molybdenum gauze, 165 mesh woven from () dia wire, twilled weave

Molybdenum Mesh AMERICAN ELEMENTS

Molybdenum (atomic symbol: Mo, atomic number: 42) is a Block D, Group 6, Period 5 element with an atomic weight of . The number of electrons in each of molybdenums shells is [2, 8, 18, 13, 1] and its electron configuration is [Kr] 4d 5 5s 1. The molybdenum atom has a radius of 139 pm and a Van der Waals radius of 209 pm.

Stainless Steel Wire Mesh Deze Wire

Best Stainless Steel Wire Mesh at supply competitiveness Stainless Steel Wire Mesh located in China. Email:Sales@

165 Mesh T316 Stainless .0019 48 Wide Wire Mesh, Mesh

Photos,prices and helpful data about 165 mesh Stainless Steel Type 316 wire screen bolting cloth with .0019 inch wire 165 Mesh T316 Stainless .0019 48 Wide

Thermo Shield Molybdenum Screen

Molybdenum refractory screen is known under many names (Mesh, Wire Cloth, Screen Grid, . Moly. Screen Twill x 12 in. wide 165 x 165 mesh x dia wire.

Molybdenum mesh, 100x100mm, nominal aperture

Molybdenum mesh, 100x100mm, nominal aperture , wire diameter mm, 26 wires/inch, open area 67%, plain weave mesh | Sigma-Aldrich

Molybdenum Wire Cloth Used for Filters, Heating Elements

Molybdenum wire cloth includes two types: silver white molybdenum mesh, black molybdenum mesh with graphite coating. Adopting plain weave, twill weave,

Pure Metal and Alloy Gauzes for Catalysis Alfa Aesar

Brass gauze, alloy 260, 20 mesh woven from () dia wire .. Molybdenum gauze, 165 mesh woven from (in) dia wire, twilled

Molybdenum Mesh online catalogue source supplier of

General Description: Discovered in 1871 by . Hjelm in Uppsala, Sweden. Molybdenum is a lustrous, silvery coloured metal which has an abundance of

Molybdenum Mill Products and Mol

A. Molybdenum Mill Products Are Available at Competitive Prices and Deliveries: Wire-mesh Moly Screen (from 165 Mesh through #2 Mesh) - Special Order.

Molybdenum Wire Mesh

464 products offers 464 molybdenum wire mesh products. About 62% of these are steel wire mesh. A wide variety of molybdenum wire mesh

Molybdenum Wire Cloth Cleveland Wire Cloth

30 Jun 2014 UNS R03610. Molybdenum wire screen is used in extremely high-temperature environments. It has good electrical conductivity, a high strength

Molybdenum Mo PubChem

Molybdenum gauze, 10 mesh woven from () dia wire .. Molybdenum gauze, 165 mesh woven from (in) dia wire, twilled