• [wzg:title/]
Inconel X750 wire

Inconel X750 wire

Inconel X750 wire

Inconel X750 / UNS N07750 / DIN W. Nr. 2.4669

 

Inconel X-750 alloy is mainly nickel-based super alloy aging with γ"[Ni3(Al, Ti, Nb)] phase. It has good corrosion resistance and oxidation resistance below 980 °C, and is higher than 800 °C. The strength, below 540 ° C has good resistance to slack, but also has good formability and weldability. The alloy is mainly used in the manufacture of aircraft engines that work below 800 ° C and require high strength and relaxation-resistant planar springs. Coil springs. Can also be used to make parts such as turbine blades

  • Bar
  • Wire
  • Sheet
  • Plate
  • Forgings
  • Pipe fittings
  • Flanges
  • Seamless & Welded pipe
  • Seamless Tube & Welded tube
  • Welding wire

 

Form

ASTM

Rod, bar and forging

ASTM B637

Chemical composition

%

Ni

Cr

Fe

C

Mn

Si

S

Ti

Nb+Ta

Al

Co

Cu

min

70

14

5

 

 

 

 

2.25

0.7

0.4

 

 

max

 

17

9

0.08

1

0.5

0.01

2.75

1.2

1

1

0.5

 

Density

8.28 g/cm3

Melting range

1393-1427

 

Application:

 

  • Nuclear reactors
  • Gas turbines
  • Rocket engines
  • Pressure vessels
  • Aircraft structures
admin@jxmatech.com

Inconel X750 / UNS N07750 / DIN W. Nr. 2.4669

 

Inconel X-750 alloy is mainly nickel-based super alloy aging with γ"[Ni3(Al, Ti, Nb)] phase. It has good corrosion resistance and oxidation resistance below 980 °C, and is higher than 800 °C. The strength, below 540 ° C has good resistance to slack, but also has good formability and weldability. The alloy is mainly used in the manufacture of aircraft engines that work below 800 ° C and require high strength and relaxation-resistant planar springs. Coil springs. Can also be used to make parts such as turbine blades

  • Bar
  • Wire
  • Sheet
  • Plate
  • Forgings
  • Pipe fittings
  • Flanges
  • Seamless & Welded pipe
  • Seamless Tube & Welded tube
  • Welding wire

 

Form

ASTM

Rod, bar and forging

ASTM B637

Chemical composition

%

Ni

Cr

Fe

C

Mn

Si

S

Ti

Nb+Ta

Al

Co

Cu

min

70

14

5

 

 

 

 

2.25

0.7

0.4

 

 

max

 

17

9

0.08

1

0.5

0.01

2.75

1.2

1

1

0.5

 

Density

8.28 g/cm3

Melting range

1393-1427

 

Application:

 

  • Nuclear reactors
  • Gas turbines
  • Rocket engines
  • Pressure vessels
  • Aircraft structures

Request a quote