Inconel 601 is an alloy material with excellent oxidation resistance at high temperature, good resistance to carbonization, good oxidation resistance, sulfur-containing atmosphere, good mechanical properties at room temperature and high temperature, good stress corrosion resistance, cracking performance due to control Carbon content and grain size, Alloy 601 has a high creep rupture strength, so it is recommended to use 601 in the field above 500 °C.

  • Inconel 601 Bar
  • Inconel 601 Wire
  • Inconel 601 Sheet
  • Inconel 601 Plate
  • Inconel 601 Forgings
  • Inconel 601 Pipe fittings
  • Inconel 601 Flanges
  • Inconel 601 Seamless & Welded pipe
  • Inconel 601 Seamless Tube & Welded tube
  • Inconel 601 Welding wire

 

Form

ASTM

Rod, bar and wire

ASTM B166

Plate, sheet and strip

ASTM B168, ASTM B906

Seamless pipe and tube

ASTM B167, ASTM B829

Welded pipe

ASTM B775

Welded tube

ASTM B751


 

ERNiCrFe-11 (Alloy 601)

AWS A5.14 ERNiCrFe-11 (UNS N06601)

ASME II, Part C, SFA-5.14, ERNiCrFe-11 (UNS N06601)

ASME IX, F-No.43

•BS290] NA 49

•DIN 1736 SG-NiCr23Al (2.4626)

•(EN) ISO 18274 - SN16601 (NiCr23Fel5Al)

'Supply to these specifications available upon request

For manufacture to ASME III (NCA3800, NB2400), AMS and other specifications

admin@jxmatech.com

Inconel 601 Welding  Wire - UNS N06601 - DIN W. Nr.2.4851

Inconel 601 Wire, Inconel 601 Spring Wire

Inconel 601 / UNS N06601 / DIN W. Nr. 2.4851

Inconel 601 is an alloy material with excellent oxidation resistance at high temperature, good resistance to carbonization, good oxidation resistance, sulfur-containing atmosphere, good mechanical properties at room temperature and high temperature, good stress corrosion resistance, cracking performance due to control Carbon content and grain size, Alloy 601 has a high creep rupture strength, so it is recommended to use 601 in the field above 500 °C.

  • Inconel 601 Bar
  • Inconel 601 Wire
  • Inconel 601 Sheet
  • Inconel 601 Plate
  • Inconel 601 Forgings
  • Inconel 601 Pipe fittings
  • Inconel 601 Flanges
  • Inconel 601 Seamless & Welded pipe
  • Inconel 601 Seamless Tube & Welded tube
  • Inconel 601 Welding wire

 

Form

ASTM

Rod, bar and wire

ASTM B166

Plate, sheet and strip

ASTM B168, ASTM B906

Seamless pipe and tube

ASTM B167, ASTM B829

Welded pipe

ASTM B775

Welded tube

ASTM B751


 

ERNiCrFe-11 (Alloy 601)

AWS A5.14 ERNiCrFe-11 (UNS N06601)

ASME II, Part C, SFA-5.14, ERNiCrFe-11 (UNS N06601)

ASME IX, F-No.43

•BS290] NA 49

•DIN 1736 SG-NiCr23Al (2.4626)

•(EN) ISO 18274 - SN16601 (NiCr23Fel5Al)

'Supply to these specifications available upon request

For manufacture to ASME III (NCA3800, NB2400), AMS and other specifications