Hastelloy C-276 / UNS N10276  / DIN W. Nr. 2.4819

 

Hastelloy C-276 is a tungsten-nickel-chromium-molybdenum alloy with a very low silicon carbon content. As a versatile corrosion-resistant alloy, mainly resistant to wet chlorine, various oxidizing chlorides, chloride solutions, sulfuric acid and oxidizing salts and have good corrosion resistance in low temperature and medium temperature hydrochloric acid.

 

  • Bar
  • Wire
  • Sheet
  • Plate
  • Forgings
  • Pipe fittings
  • Flanges
  • Seamless & Welded pipe
  • Seamless Tube & Welded tube
  • Welding Wire

 

 

Form

ASTM

Rod

ASTM B574

Plate, sheet and strip

ASTM B575

Seamless pipe and tube

ASTM B622

Welded pipe

ASTM B619, ASTM B775

Welded tube

ASTM B626, ASTM B751

Welding fitting

ASTM B366

Forged or rolled pipe flange and forged fitting

ASTM B462

Billet and bar for reforging

ASTM B472

Forging

ASTM B564


 

Chemical composition

%

Ni

Cr

Mo

Fe

W

Co

C

Mn

Si

P

S

V

min

balance

20

12.5

2

2.5

 

 

 

 

 

 

 

max

22.5

14.5

6

3.5

2.5

0.015

0.5

0.08

0.02

0.02

0.35

 

Application:

  • Pollution control
  • Chemical processing
  • Pulp & paper production
  • Waste treatment
admin@jxmatech.com

Hastelloy C-276 / UNS N10276  / DIN W. Nr. 2.4819

 

Hastelloy C-276 is a tungsten-nickel-chromium-molybdenum alloy with a very low silicon carbon content. As a versatile corrosion-resistant alloy, mainly resistant to wet chlorine, various oxidizing chlorides, chloride solutions, sulfuric acid and oxidizing salts and have good corrosion resistance in low temperature and medium temperature hydrochloric acid.

 

  • Bar
  • Wire
  • Sheet
  • Plate
  • Forgings
  • Pipe fittings
  • Flanges
  • Seamless & Welded pipe
  • Seamless Tube & Welded tube
  • Welding Wire

 

 

Form

ASTM

Rod

ASTM B574

Plate, sheet and strip

ASTM B575

Seamless pipe and tube

ASTM B622

Welded pipe

ASTM B619, ASTM B775

Welded tube

ASTM B626, ASTM B751

Welding fitting

ASTM B366

Forged or rolled pipe flange and forged fitting

ASTM B462

Billet and bar for reforging

ASTM B472

Forging

ASTM B564


 

Chemical composition

%

Ni

Cr

Mo

Fe

W

Co

C

Mn

Si

P

S

V

min

balance

20

12.5

2

2.5

 

 

 

 

 

 

 

max

22.5

14.5

6

3.5

2.5

0.015

0.5

0.08

0.02

0.02

0.35

 

Application:

  • Pollution control
  • Chemical processing
  • Pulp & paper production
  • Waste treatment

Request a quote