Hastelloy C-276 / UNS N10276  / DIN W. Nr. 2.4819

Hastelloy C 276 Pipe fittings ( Short Radius Elbows , Long Radius Elbows , Concentric Reducers , Eccentric Reducers , Stub Ends , End Caps , Equal Tees , Weldolets , Pipe Nipples .)

Hastelloy Alloy C-276 Pipe Fittings Specification

Specifications ASTM B366 / ASME SB366

Dimensions ASME/ANSI B16.9, ASME B16.28, MSS-SP-43, MSS SP-79

Size 1/8” NB TO 48” NB. (Seamless & 100% X-Ray Welded, Fabricated)

Type Seamless / Welded / Fabricated

Bending Radius R=1D, 2D, 3D, 5D, 6D, 8D, 10D or Custom

Thickness Sch 5s, Sch 10s, Sch 40s, Sch 80s, Sch 160s, Sch XXS

Grade Hastelloy C276 Pipe Fittings UNS (N10276), DIN (2.4819)

  • Hastelloy C 276 Bar
  • Hastelloy C 276 Wire
  • Hastelloy C 276 Sheet
  • Hastelloy C 276 Plate
  • Hastelloy C 276 Forgings
  • Hastelloy C 276 Pipe fittings
  • Hastelloy C 276 Flanges
  • Hastelloy C 276 Seamless & Welded pipe
  • Hastelloy C 276 Seamless Tube & Welded tube
  • Hastelloy C 276 Welding Wire

 

Form

ASTM

Rod

ASTM B574

Plate, sheet and strip

ASTM B575

Seamless pipe and tube

ASTM B622

Welded pipe

ASTM B619, ASTM B775

Welded tube

ASTM B626, ASTM B751

Welding fitting

ASTM B366

Forged or rolled pipe flange and forged fitting

ASTM B462

Billet and bar for reforging

ASTM B472

Forging

ASTM B564

 

Chemical composition

%

Ni

Cr

Mo

Fe

W

Co

C

Mn

Si

P

S

V

min

balance

20

12.5

2

2.5

 

 

 

 

 

 

 

max

22.5

14.5

6

3.5

2.5

0.015

0.5

0.08

0.02

0.02

0.35

 

Application:

  • Pollution control
  • Chemical processing
  • Pulp & paper production
  • Waste treatment


 

admin@jxmatech.com

Hastelloy C-276 / UNS N10276  / DIN W. Nr. 2.4819

Hastelloy C 276 Pipe fittings ( Short Radius Elbows , Long Radius Elbows , Concentric Reducers , Eccentric Reducers , Stub Ends , End Caps , Equal Tees , Weldolets , Pipe Nipples .)

Hastelloy Alloy C-276 Pipe Fittings Specification

Specifications ASTM B366 / ASME SB366

Dimensions ASME/ANSI B16.9, ASME B16.28, MSS-SP-43, MSS SP-79

Size 1/8” NB TO 48” NB. (Seamless & 100% X-Ray Welded, Fabricated)

Type Seamless / Welded / Fabricated

Bending Radius R=1D, 2D, 3D, 5D, 6D, 8D, 10D or Custom

Thickness Sch 5s, Sch 10s, Sch 40s, Sch 80s, Sch 160s, Sch XXS

Grade Hastelloy C276 Pipe Fittings UNS (N10276), DIN (2.4819)

  • Hastelloy C 276 Bar
  • Hastelloy C 276 Wire
  • Hastelloy C 276 Sheet
  • Hastelloy C 276 Plate
  • Hastelloy C 276 Forgings
  • Hastelloy C 276 Pipe fittings
  • Hastelloy C 276 Flanges
  • Hastelloy C 276 Seamless & Welded pipe
  • Hastelloy C 276 Seamless Tube & Welded tube
  • Hastelloy C 276 Welding Wire

 

Form

ASTM

Rod

ASTM B574

Plate, sheet and strip

ASTM B575

Seamless pipe and tube

ASTM B622

Welded pipe

ASTM B619, ASTM B775

Welded tube

ASTM B626, ASTM B751

Welding fitting

ASTM B366

Forged or rolled pipe flange and forged fitting

ASTM B462

Billet and bar for reforging

ASTM B472

Forging

ASTM B564

 

Chemical composition

%

Ni

Cr

Mo

Fe

W

Co

C

Mn

Si

P

S

V

min

balance

20

12.5

2

2.5

 

 

 

 

 

 

 

max

22.5

14.5

6

3.5

2.5

0.015

0.5

0.08

0.02

0.02

0.35

 

Application:

  • Pollution control
  • Chemical processing
  • Pulp & paper production
  • Waste treatment


 

Request a quote