• [wzg:title/]
Hastelloy C22 Pipe fittings

Hastelloy C22 Pipe fittings

Hastelloy C22 Pipe fittings

Hastelloy C-22 / UNS N06022  / DIN W. Nr. 2.4602

Hastelloy C 22 Pipe fittings ( Short Radius Elbows , Long Radius Elbows , Concentric Reducers , Eccentric Reducers , Stub Ends , End Caps , Equal Tees , Weldolets , Pipe Nipples .)

  • Hastelloy C22 Bar
  • Hastelloy C22 Wire
  • Hastelloy C22 Sheet
  • Hastelloy C22 Plate
  • Hastelloy C22 Forgings
  • Hastelloy C22 Pipe fittings
  • Hastelloy C22 Flanges
  • Hastelloy C22 Seamless & Welded pipe
  • Hastelloy C22 Seamless Tube & Welded tube
  • Hastelloy C22 Weld Wire

Hastelloy Alloy C-22 Pipe Fittings Specification

Specifications ASTM B366 / ASME SB366

Dimensions ASME/ANSI B16.9, ASME B16.28, MSS-SP-43, MSS SP-79

Size 1/8” NB TO 48” NB. (Seamless & 100% X-Ray Welded, Fabricated)

Type Seamless / Welded / Fabricated

Bending Radius R=1D, 2D, 3D, 5D, 6D, 8D, 10D or Custom

Thickness Sch 5s, Sch 10s, Sch 40s, Sch 80s, Sch 160s, Sch XXS

Grade Hastelloy C276 Pipe Fittings UNS (N10276), DIN (2.4819)

 

Form

ASTM

Rod

B 574

Plate, sheet and strip

B 575

Seamless pipe and tube

B 622

Welded pipe

B 619, B 775

Welded tube

B 626, B 751

Welding fitting

B 366

Forged or rolled pipe flange and forged fitting

B 462

Billet and bar for reforging

B 472

Forging

B 564

Chemical composition

%

Ni

Cr

Mo

Fe

W

Co

C

Mn

Si

P

S

V

min

balance

20

12.5

2

2.5

 

 

 

 

 

 

 

max

22.5

14.5

6

3.5

2.5

0.015

0.5

0.08

0.02

0.02

0.35

 

Density

8.69 g/cm3

Melting range

1325-1370

 

Application:

  • Marine
  • Power
  • Chemical processing
  • Pollution control
  • Paper processing


 

admin@jxmatech.com

Hastelloy C-22 / UNS N06022  / DIN W. Nr. 2.4602

Hastelloy C 22 Pipe fittings ( Short Radius Elbows , Long Radius Elbows , Concentric Reducers , Eccentric Reducers , Stub Ends , End Caps , Equal Tees , Weldolets , Pipe Nipples .)

  • Hastelloy C22 Bar
  • Hastelloy C22 Wire
  • Hastelloy C22 Sheet
  • Hastelloy C22 Plate
  • Hastelloy C22 Forgings
  • Hastelloy C22 Pipe fittings
  • Hastelloy C22 Flanges
  • Hastelloy C22 Seamless & Welded pipe
  • Hastelloy C22 Seamless Tube & Welded tube
  • Hastelloy C22 Weld Wire

Hastelloy Alloy C-22 Pipe Fittings Specification

Specifications ASTM B366 / ASME SB366

Dimensions ASME/ANSI B16.9, ASME B16.28, MSS-SP-43, MSS SP-79

Size 1/8” NB TO 48” NB. (Seamless & 100% X-Ray Welded, Fabricated)

Type Seamless / Welded / Fabricated

Bending Radius R=1D, 2D, 3D, 5D, 6D, 8D, 10D or Custom

Thickness Sch 5s, Sch 10s, Sch 40s, Sch 80s, Sch 160s, Sch XXS

Grade Hastelloy C276 Pipe Fittings UNS (N10276), DIN (2.4819)

 

Form

ASTM

Rod

B 574

Plate, sheet and strip

B 575

Seamless pipe and tube

B 622

Welded pipe

B 619, B 775

Welded tube

B 626, B 751

Welding fitting

B 366

Forged or rolled pipe flange and forged fitting

B 462

Billet and bar for reforging

B 472

Forging

B 564

Chemical composition

%

Ni

Cr

Mo

Fe

W

Co

C

Mn

Si

P

S

V

min

balance

20

12.5

2

2.5

 

 

 

 

 

 

 

max

22.5

14.5

6

3.5

2.5

0.015

0.5

0.08

0.02

0.02

0.35

 

Density

8.69 g/cm3

Melting range

1325-1370

 

Application:

  • Marine
  • Power
  • Chemical processing
  • Pollution control