Application

Heating Resistors are used as heating components to plate the substrates of kinescope,mirrors,plastics,metal and various decorations.Stranded wires are used as raw material of heating elements,and also as heating components of semiconductors and vacuum devices directly.

Features

With special equipment,Heating Resistors made from tungsten wire HW41 is of high melting point,good corrosion resistance,and long life.Metal wire to be used as coating material can also be stranded round tungsten wire,which will be more convenient and efficient for further process.

State of Finished Products

Sizes:Φ0.3~1.5mm×n(n≤10);

Surface:Chemical cleaned or Electrolytic Polishde;

Technical requirements:As per the drawings provide by customers,or Xiamen Honglu standard"tungsten Heating Resistors for Metallization Q/XHL02-2004".

admin@jxmatech.com

Stranded Tungsten Wire,Heating Resistors

Application

Heating Resistors are used as heating components to plate the substrates of kinescope,mirrors,plastics,metal and various decorations.Stranded wires are used as raw material of heating elements,and also as heating components of semiconductors and vacuum devices directly.

Features

With special equipment,Heating Resistors made from tungsten wire HW41 is of high melting point,good corrosion resistance,and long life.Metal wire to be used as coating material can also be stranded round tungsten wire,which will be more convenient and efficient for further process.

State of Finished Products

Sizes:Φ0.3~1.5mm×n(n≤10);

Surface:Chemical cleaned or Electrolytic Polishde;

Technical requirements:As per the drawings provide by customers,or Xiamen Honglu standard"tungsten Heating Resistors for Metallization Q/XHL02-2004".