• [wzg:title/]
Alloy 52 Bar

Alloy 52 Bar

Alloy 52 Bar

 

Alloy 52 bar / N14052 Alloy 52 contains 52% nickel and 48% iron and is widely used in the telecommunications industry. It also finds application in a wide variety of electronic applications, especially for glass seals.

Also known as: Pernifer 502, NILO 50, Glass Seal 521

 

  • Bar
  • Wire
  • Sheet
  • Plate
  • Forgings
  • Foil

Applications

Glass to metal seals for electronic tubes

Automotive and industrial lamps

Specialty hermetic devices

 

Alloy Type

Trade Name

UNS No.

Standard

Forms

Rod

Strip

Wire

Sheet

Ni29Co17

Kovar

K94610

ASTM F15

?

?

?

?

FeNi36

Invar 36

K93603

ASTM 1684

?

?

?

 

FeNi32Co5

Super-invar 32-5

K93500

ASTM F1684

?

?

?

 

FeNi33Co17

Ni33Co17

?

YB/T5234-94

?

?

?

?

FeNi27Co25

Ceramvar

F1466

ASTM F1466

?

?

?

?

Fe28Cr

Alloy 27

K92801

ASTM F256

?

?

?

 

Fe42Ni6Cr

Alloy 426

K94760

ASTM F31

?

?

?

 

Fe42Ni

Alloy 42

K94100

ASTM F30

?

?

?

 

Fe45Ni

Alloy45

?

YB/5235-2005

?

?

?

 

Fe46Ni

Alloy46

K94600

ASTM F30

?

?

?

 

Fe50Ni

Alloy52

K95050

ASTM F30

?

?

?

 

admin@jxmatech.com

 

Alloy 52 bar / N14052 Alloy 52 contains 52% nickel and 48% iron and is widely used in the telecommunications industry. It also finds application in a wide variety of electronic applications, especially for glass seals.

Also known as: Pernifer 502, NILO 50, Glass Seal 521

 

  • Bar
  • Wire
  • Sheet
  • Plate
  • Forgings
  • Foil

Applications

Glass to metal seals for electronic tubes

Automotive and industrial lamps

Specialty hermetic devices

 

Alloy Type

Trade Name

UNS No.

Standard

Forms

Rod

Strip

Wire

Sheet

Ni29Co17

Kovar

K94610

ASTM F15

?

?

?

?

FeNi36

Invar 36

K93603

ASTM 1684

?

?

?

 

FeNi32Co5

Super-invar 32-5

K93500

ASTM F1684

?

?

?

 

FeNi33Co17

Ni33Co17

?

YB/T5234-94

?

?

?

?

FeNi27Co25

Ceramvar

F1466

ASTM F1466

?

?

?

?

Fe28Cr

Alloy 27

K92801

ASTM F256

?

?

?

 

Fe42Ni6Cr

Alloy 426

K94760

ASTM F31

?

?

?

 

Fe42Ni

Alloy 42

K94100

ASTM F30

?

?

?

 

Fe45Ni

Alloy45

?

YB/5235-2005

?

?

?

 

Fe46Ni

Alloy46

K94600

ASTM F30

?

?

?

 

Fe50Ni

Alloy52

K95050

ASTM F30

?

?

?

 

Request a quote