Alloy 46 Sheet: Consisting of 46% nickel and iron balance, 46 Alloy is a controlled expansion alloy used mostly in electronic applications, especially for glass and ceramic seals. Alloy 46 is also known as Pernifer 462, NILO 464, and Glass-Seal 461

  • Bar
  • Wire
  • Sheet
  • Plate
  • Forgings
  • Foil


 

Alloy Type

Trade Name

UNS No.

Standard

Forms

Rod

Strip

Wire

Sheet

Ni29Co17

Kovar

K94610

ASTM F15

Y

Y

Y

Y

FeNi36

Invar 36

K93603

ASTM 1684

Y

Y

Y

 

FeNi32Co5

Super-invar 32-5

K93500

ASTM F1684

Y

Y

Y

 

FeNi33Co17

Ni33Co17

 

YB/T5234-94

Y

Y

Y

Y

FeNi27Co25

Ceramvar

F1466

ASTM F1466

Y

Y

Y

Y

Fe28Cr

Alloy 27

K92801

ASTM F256

Y

Y

Y

 

Fe42Ni6Cr

Alloy 426

K94760

ASTM F31

Y

Y

Y

 

Fe42Ni

Alloy 42

K94100

ASTM F30

Y

Y

Y

 

Fe45Ni

Alloy45

 

YB/5235-2005

Y

Y

Y

 

Fe46Ni

Alloy46

K94600

ASTM F30

Y

Y

Y

 

Fe50Ni

Alloy52

K95050

ASTM F30

Y

Y

Y

 

 

admin@jxmatech.com

Alloy 46 Sheet: Consisting of 46% nickel and iron balance, 46 Alloy is a controlled expansion alloy used mostly in electronic applications, especially for glass and ceramic seals. Alloy 46 is also known as Pernifer 462, NILO 464, and Glass-Seal 461

  • Bar
  • Wire
  • Sheet
  • Plate
  • Forgings
  • Foil


 

Alloy Type

Trade Name

UNS No.

Standard

Forms

Rod

Strip

Wire

Sheet

Ni29Co17

Kovar

K94610

ASTM F15

Y

Y

Y

Y

FeNi36

Invar 36

K93603

ASTM 1684

Y

Y

Y

 

FeNi32Co5

Super-invar 32-5

K93500

ASTM F1684

Y

Y

Y

 

FeNi33Co17

Ni33Co17

 

YB/T5234-94

Y

Y

Y

Y

FeNi27Co25

Ceramvar

F1466

ASTM F1466

Y

Y

Y

Y

Fe28Cr

Alloy 27

K92801

ASTM F256

Y

Y

Y

 

Fe42Ni6Cr

Alloy 426

K94760

ASTM F31

Y

Y

Y

 

Fe42Ni

Alloy 42

K94100

ASTM F30

Y

Y

Y

 

Fe45Ni

Alloy45

 

YB/5235-2005

Y

Y

Y

 

Fe46Ni

Alloy46

K94600

ASTM F30

Y

Y

Y

 

Fe50Ni

Alloy52

K95050

ASTM F30

Y

Y

Y

 

 