Alloy 42 Sheet

Alloy 42 Sheet

Alloy 42 Sheet

Alloy 42 Sheet  Nilo 42 (UNS K94100 /ASTM F30 / 1.3917)

Grade: 4J42|Nilo 42|FeNi42|K94100|Alloy 42

>Uses: It is used to make iron-nickel alloy strips, bars, tubes, wires and plates with electrical glass and ceramics. In the electric vacuum industry, the corresponding soft glass is matched and sealed.

 

Grade Relative Grade
  Russia U.S.A. U.K.   France Germany
  Н42 X 6 42Ni-6Cr
Carpenter426
Sylvania4
Sealmet 4
-   ASV(426)
Ni42Cr6
Vacovit426
(NiCr426)
  47НХ - -   461 -
  49НХР Carpenter 456 -   FeNi47Cr6 Vacovit 465
Alloy 42  42Н Glass Sealing 42
Uniseal 42
Nilo42   N42 Vacodil 42
Nilo42
Alloy 45 46Н Niromet 46
Ferrovac 46 Ni
Nilo45   Fe-Ni42 Vacodil 46
Alloy 52 50Н FeNi50 Nilo51   N50 Vacovit 500
  52Н
50Н-ВИ
Glass Sealing 52
Niloy 52
-   N52 Vacovit 520
FeNi52
  - - -   N54 Vacovit 540
FeNi54

Alloy 42 belong to a controlled expansion alloy Similar called: 4J42, Nio 42, NI42 Fe42Ni (UNS K94100 /ASTM F30) (aka Pernifer 402, NILO 424, Glass Seal 421). 


 

admin@jxmatech.com

Alloy 42 Sheet  Nilo 42 (UNS K94100 /ASTM F30 / 1.3917)

Grade: 4J42|Nilo 42|FeNi42|K94100|Alloy 42

>Uses: It is used to make iron-nickel alloy strips, bars, tubes, wires and plates with electrical glass and ceramics. In the electric vacuum industry, the corresponding soft glass is matched and sealed.

 

Grade Relative Grade
  Russia U.S.A. U.K.   France Germany
  Н42 X 6 42Ni-6Cr
Carpenter426
Sylvania4
Sealmet 4
-   ASV(426)
Ni42Cr6
Vacovit426
(NiCr426)
  47НХ - -   461 -
  49НХР Carpenter 456 -   FeNi47Cr6 Vacovit 465
Alloy 42  42Н Glass Sealing 42
Uniseal 42
Nilo42   N42 Vacodil 42
Nilo42
Alloy 45 46Н Niromet 46
Ferrovac 46 Ni
Nilo45   Fe-Ni42 Vacodil 46
Alloy 52 50Н FeNi50 Nilo51   N50 Vacovit 500
  52Н
50Н-ВИ
Glass Sealing 52
Niloy 52
-   N52 Vacovit 520
FeNi52
  - - -   N54 Vacovit 540
FeNi54

Alloy 42 belong to a controlled expansion alloy Similar called: 4J42, Nio 42, NI42 Fe42Ni (UNS K94100 /ASTM F30) (aka Pernifer 402, NILO 424, Glass Seal 421). 


 